Process for producing aluminate-based phosphor
AssigneeSumitomo Chemical Company, Limited
InventorsKeiji Ono, Susumu Miyazaki
Life of this patent
Estimating the term…
Abstract
The present invention provides a method for producing an aluminate-based phosphor or a luminescent aluminate-based phosphor, which comprises calcining an aluminum compound having a BET specific surface area of 100 m2/g or more.
Claims23
A method for producing an aluminate-based phosphor comprising mixing an aluminum compound and a metal compound and calcining the mixture, wherein the aluminum compound has a BET specific surface area of 100 m2/g or more and the aluminate-based phosphor comprises the metal of the metal compound.
A method for producing an aluminate-based phosphor comprising the steps of;
- mixing an aluminum compound with an organic acid using an organic solvent to obtain a slurry,
- mixing the slurry with an aqueous solution of at least one cation selected from the group consisting of Ba, Mg, Eu, Mn, Sr, Ca, Tb, Ce and Zn to obtain a slurry of the mixture,
- precipitating the cation in the form of an organic acid salt around the aluminum compound to obtain a precursor,
- separating and drying the precursor, and
- calcining the precursor at a temperature of from 1000° C. or more to 1700° C. or less, to produce an aluminate-based phosphor.
A method for producing a luminescent aluminate-based phosphor comprising mixing an aluminum compound and a metal compound and calcining the mixture, wherein the aluminum compound has a BET specific surface area of 100 m2/g or more and the luminescent aluminate-based phosphor comprises the metal of the metal compound and wherein the luminescent aluminate-based phosphor has an afterglow brilliance.
A method for producing a luminescent aluminate-based phosphor comprising the steps of;
- mixing an aluminum compound with an organic acid using an organic solvent to obtain a slurry,
- mixing the slurry with an aqueous solution of at least one cation selected from the group consisting of Eu, Dy, Nd, Sr, Ca, Pb, Zn and Bi to obtain a slurry of the mixture,
- precipitating the cation in the form of an organic acid salt around the aluminum compound to obtain a precursor,
- separating and drying the precursor, and
- calcining the precursor at a temperature of from 1000° C. or more to 1700° C. or less, to produce an aluminate-based phosphor.