Thermoplastically processable polyurethane elastomers having an improved intrinsic color
AssigneeBayer Aktiengesellschaft
InventorsWolfgang Bräuer, Wolfgang Kaufhold, Hans-Georg Hoppe, Hans-Georg Wussow
Life of this patent
Estimating the term…
Abstract
A light-colored thermoplastic molding composition comprising a polyurethane elastomer is disclosed. The polyurethane which is the reaction product of at least one polyol, at least one organic diisocyanate and at least one polyol chain extender contains one or more pentaerythritol diphosphites color stabilizers conforming to a specific formula exhibits improved color stability and improved processability. The process for preparation entails introducing the stabilizer before the reaction has been completed.
Claims14
A light-colored thermoplastic molding composition comprising the reaction product of A, B and C where
- A) is at least one polyol having on average 1.8 to 3.0 Zerewitinoff-active hydrogen atoms and a number average molecular weight of 450 to 10,000, and
- B) is at least one organic diisocyanate and
- C) is at least one polyol having on average 1.8 to 3.0 Zerewitinoff-active hydrogen atoms and a number average molecular weight of 60 to 400,
- wherein the ratio NCO/OH of A), B) and C) is between 0.85 and 1.2 to obtain a polyurethane elastomer,
- and 0 to 20% of an auxiliary substance or additive (D), and
- 0.001 to 1%, of one or more color stabilizers (E) selected from the group consisting of pentaerythritol diphosphites corresponding to the formula (I)
- wherein
- R is C6 to C30-alkyl and Ph denotes phenyl, said percents, both occurrences, being in relation to the weight of the elastomer.
A process for preparing a light-colored thermoplastic molding composition comprising the product of the reaction of A, B and C where
- A) is at least one polyol having on average 1.8 to 3.0 Zerewitinoff-active hydrogen atoms and a number average molecular weight of 450 to 10,000, and
- B) is at least one organic diisocyanate and
- C) is at least one polyol having on average 1.8 to 3.0 Zerewitinoff-active hydrogen atoms and a number average molecular weight of 60 to 400,
- wherein the ratio NCO/OH of A), B) and C) is between 0.85 and 1.2 to obtain a polyurethane elastomer,
- and introducing to the reaction before it has been completed 0.001 to 1%, in relation to the weight of said A, B and C, of one or more color stabilizers E, selected from the group consisting of pentaerythritol diphosphites corresponding to the formula (I)
- wherein
- R is C6 to C30-alkyl and Ph denotes phenyl.