Process for modifying particle size distribution
AssigneeThiele Kaolin Company
InventorsR. Andrew Lowe, Prakash B. Malla, William M. McClarin III, Don R. Black
Life of this patent
Estimating the term…
Abstract
Fine-grained Tertiary kaolin clay pigments providing improved opacity, sheet gloss and print gloss to paper coated with these pigments are produced by removing fine and coarse particles to produce pigments having a narrow particle size distribution.
Claims7
A process for modifying the particle size distribution of a fine-grained Tertiary kaolin clay, wherein the process comprises the sequential steps of:
- A. obtaining a starting material comprising an aqueous slurry of a dispersed and degritted fine-grained Tertiary kaolin clay;
- and
- B. tailoring the slurry by removing (a) a portion of particles having an e.s.d. less than 0.2 microns and (b) particles having an e.s.d. greater than 2.0 microns,
- thereby producing a pigment having a particle size distribution of 90-100 percent by weight less than 2.0 microns e.s.d. and at least 15 percent by weight less than 0.2 microns e.s.d.
A tailored pigment comprising a fine-grained Tertiary kaolin clay and having a particle size distribution of:
- 90-100 percent by weight less than 2.0 microns e.s.d
- 80-100 percent by weight less than 1.0 microns e.s.d.
- 55-90 percent by weight less than 0.5 microns e.s.d.
- 30-60 percent by weight less than 0.3 microns e.s.d.
- 15-35 percent by weight less than 0.2 microns e.s.d.
A tailored pigment comprising a fine-grained Tertiary kaolin clay and having a particle size distribution of:
- 95-100 percent by weight less than 2.0 microns e.s.d
- 85-100 percent by weight less than 1.0 microns e.s.d.
- 65-90 percent by weight less than 0.5 microns e.s.d.
- 30-50 percent by weight less than 0.3 microns e.s.d.
- 15-25 percent by weight less than 0.2 microns e.s.d.
Dependencies are inferred from the claim text.