# US 6,440,653 B2 · Method of producing a photographic image

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,440,653 B2
- Document ID: US6440653B2
- Status: Granted
- Kind: B2
- Application number: 09/852,368
- Filed: 2001-05-10
- Published: 2002-02-07
- Granted: 2002-08-27
- Earliest claimed: 2000-06-28
- Assignees: Eastman Kodak Company
- Inventors: John R. Fyson; Louis E. Friedrich
- Web page: https://patentgrep.com/patent/US6440653B2

## CPC

- G03C 7/3046: {Processing baths not provided for elsewhere, e.g. final or intermediate washings}
- G03C 5/268: {Processing baths not provided for elsewhere, e.g. pre-treatment, stop, intermediate or rinse baths (colour processing G03C7/3046)}
- G03C 7/3017: {with intensification of the image by oxido-reduction}
- Y10S 430/144: Hydrogen peroxide treatment
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method of producing a photographic image in an imagewise exposed photographic material comprising one or more silver halide emulsion layers comprises developing the material with a developer solution containing a silver halide developing agent, applying to the surface of the developed material a solution of a sulphite compound that reacts with oxidised developing agent and prevents further development, and applying to the surface of the developed material a solution of an oxidant that oxidises any remaining developing agent, wherein said sulphite compound is present in an amount sufficient to react with all the oxidised developing agent and said solutions of sulphite and oxidant are applied to the material by means other than immersion in a tank.

## Claims

### Claim 1

A method of producing a photographic image in an imagewise exposed photographic material comprising one or more silver halide emulsion layers which method comprises
developing the material with a developer solution containing a silver halide developing agent,
applying to the surface of the developed material a solution of a sulphite compound that reacts with oxidised developing agent and prevents further development, and
applying to the surface of the developed material a solution of an oxidant that oxidises any remaining developing agent,
wherein said sulphite compound is present in an amount sufficient to react with all the oxidised developing agent and said solutions of sulphite and oxidant are applied to the material by means other than immersion in a tank.

### Claim 2 (depends on 1)

A method as claimed in claim 1 wherein the photographic material is a colour photographic material.

### Claim 3 (depends on 1)

A method as claimed in claim 1 wherein development is accompanied by an amplification step.

### Claim 4 (depends on 1)

A method as claimed in claim 1 wherein the sulphite compound is a hydrogen sulphite or metabisulphite compound.

### Claim 5 (depends on 1)

A method as claimed in claim 1 wherein the sulphite compound is present in an amount from 0.02 to 1 mole/l.

### Claim 6 (depends on 1)

A method as claimed in claim 1 wherein the oxidant is a salt of a peroxy sulphuric acid.

### Claim 7 (depends on 1)

A method as claimed in claim 1 wherein the oxidant is present in an amount from 0.02 to 1 mole/l.

### Claim 8 (depends on 1)

A method as claimed in claim 1 wherein said solutions of sulphite and oxidant are applied to the material by spraying from a fine nozzle, an air brush, an ink jet head or by application with a roller.

### Claim 9 (depends on 1)

A method as claimed in claim 1 wherein the total amount of said solutions of sulphite and oxidant applied to the surface of the developed material does not exceed 100 ml/m2.

### Claim 10 (depends on 1)

A method as claimed in claim 1 wherein the total amount of said solutions of sulphite and oxidant applied to the surface of the developed material is from 20 to 60 ml/m2.