Fluid compression of injection molded plastic materials
AssigneeIncoe Corporation
InventorsTristan Seres, John D. Blundy, James W. Hendry
Life of this patent
Estimating the term…
Abstract
An injection mold apparatus having two halves, a core portion and a cavity portion. One or more gas injection devices, such as porous metal devices, are located in either of the two portions of the mold. Once a charge of hot melted plastic is injected into the mold cavity, gas is injected through gas injection devices forcing the hot plastic against the opposite mold half and into any recesses and grooves. Gas seals are formed by the plastic to prevent gas in the mold cavity from reaching the exterior surface of the molded part during shrinkage of the plastic. The centers of mass of the plastic at rib intersections are optimally positioned to eliminate sink marks on the external finished surfaces of the molded parts.
Claims9
A method of injection molding a plastic product having a first wall member with an outer appearance surface and a backside surface and a first reinforcing rib member positioned on said backside surface, the method comprising the steps of:
- providing a mold cavity;
- injecting a molten plastic material into the mold cavity;
- injecting gas into the mold cavity along said backside surface of the plastic material and forcing the outer appearance side of the plastic material against a first surface of the mold cavity;
- positioning the center of mass of the plastic material in said first wall member adjacent said first reinforcing rib member closer to the outer appearance surface of the molded product then the backside surface of the molded product, wherein the formation of sink marks on the outer appearance surface of the plastic product opposite said first reinforcing rib member are avoided;
- wherein the intersection of the first wall member and the first reinforcing rib member is substantially at right angles, with the intersection having radii of less than 1.0 mm.
A method of injection molding a plastic product having a first wall member with an outer appearance surface and a backside surface and a first reinforcing rib member positioned on said backside surface, the method comprising the steps of:
- providing a mold cavity;
- injecting a molten plastic material into the mold cavity;
- injecting gas into the mold cavity along said backside surface of the plastic material and forcing the outer appearance side of the plastic material against a first surface of the mold cavity;
- positioning the center of mass of the plastic material in said first wall member adjacent said first reinforcing rib member closer to the outer appearance surface of the molded product then the backside surface of the molded product, wherein the formation of sink marks on the outer appearance surface of the plastic product opposite said first reinforcing rib member are avoided;
- wherein the center of mass is positioned at a closer distance at least 50% of the distance between said outer appearance surface of the molded product than the backside of the molded product.
Dependencies are inferred from the claim text.