# US 6,417,481 B2 · Method and a device for heating at least two elements by means of laser beams of high energy density

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,417,481 B2
- Document ID: US6417481B2
- Status: Granted
- Kind: B2
- Application number: 09/746,285
- Filed: 2000-12-22
- Published: 2001-09-06
- Granted: 2002-07-09
- Earliest claimed: 1999-12-23
- Assignees: Leister Process Technologies
- Inventors: Jie-Wei Chen; Christiane Leister
- Web page: https://patentgrep.com/patent/US6417481B2

## CPC

- B29C 65/1674: {making use of laser diodes (B29C65/167 takes precedence)}
- B23K 26/066: by using masks
- B29C 65/1654: {scanning at least one of the parts to be joined}
- B29C 65/1696: {making use of masks}
- B29C 66/1122: {Single lap to lap joints, i.e. overlap joints (B29C66/45, B29C66/472, B29C66/52272 take precedence)}
- B29C 66/24245: {forming a square}
- B29C 66/244: {said joint lines being non-straight, e.g. forming non-closed contours}
- B29C 66/306: {Applying a mark during joining}
- B29C 66/41: {Joining substantially flat articles (B29C66/47 and subgroups take precedence); Making flat seams in tubular or hollow articles (B29C66/51 and subgroups take precedence)}
- B29C 66/836: {Moving relative to and tangentially to the parts to be joined, e.g. transversely to the displacement of the parts to be joined, e.g. using a X-Y table (B29C66/65 takes precedence)}
- B29C 65/1635: {at least passing through one of the parts to be joined, i.e. laser transmission welding}
- B29C 66/242: {said joint lines being closed, i.e. forming closed contours}
- B29C 66/73921: {characterised by the materials of both parts being thermoplastics}
- B29C 66/80: {General aspects of machine operations or constructions and parts thereof}
- B29K 2995/0027: for light outside the visible spectrum
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A process and a device for joining or separating various workpieces, in particular made of plastic or plastic and other materials, by means of curtain-like laser beams. To join workpieces in a particular joining area of the contact surface, a mask, made of a laser-impermeable material, is arranged between the laser source and the workpieces to be joined. The laser beam and the mask are moved relative to each other. To generate high energy density in the joining area, laser beams of at least two diode lasers are brought together, and subsequently, differing laser line lengths are generated by means of a zoom optics arrangement. Via a beam splitter, a first laser beam aligned perpendicularly to the surface of the mask, is joined by at least one secondary laser beam arranged perpendicularly to the first laser beam, and the resulting laser beam is directed onto the mask.

## Claims

### Claim 1

A method which comprises: selective heating of at least two materials by means of laser beams, with a mask made of a material impermeable to radiation arranged between a radiation source and the materials; removing regions from said mask, with the laser radiation being admitted through said regions to selected heating regions of the materials arranged below the mask; wherein all heating regions are heated by irradiation, thus leading to joining or separation of the materials, with a relative movement between one or several laser beams and the materials being carried out, and wherein for generating a high energy density, laser beams from at least two diode lasers are brought together into the heating region and with different laser line lengths being subsequently generated by means of zoom optics.

### Claim 2 (depends on 1)

A method according to claim 1, wherein a first laser beam is aligned perpendicularly to the surface of the mask, is joined by at least one secondary laser beam arranged perpendicularly to the first laser beam, with such joining or admixing taking place via a beam splitter for each secondary laser beam, and with a resulting laser beam being directed onto the joining area.

### Claim 3 (depends on 2)

A method according to claim 2, wherein laser beams either of different wavelengths or of the same wavelength but of different polarisation are used.

### Claim 4 (depends on 1)

A method according to claim 1, wherein several laser beams are focussed parallel to each other onto the joining area by means of a lens.

### Claim 5

A method which comprises: joining various workpieces made of one of (1) plastic and (2) plastic and other materials, with an upper workpiece facing a laser source for a laser beam; wherein said upper workpiece is a material which is transparent to the laser beam, and a second workpiece comprises a material which is absorbent to the laser beam so that the adjoining contact surfaces of the two workpieces melt and connect during subsequent cooling under pressure; arranging a mask made of a laser impermeable material between the laser source and the workpieces to be connected so as to connect the workpieces in a particular joining area of the contact surface; wherein the structures of said mask are larger than the wavelength of the laser beam applied; and wherein the laser source is set to the contact surface in such a way that a curtain-like laser beam is formed and that a line results at the contact surface, and that the laser beam and the mask are moved relative to each other; and wherein for generating high energy density in the joining area, laser beams of at least two diode lasers are brought together, and that subsequently, different laser line lengths are generated by means of zoom optics.

### Claim 6 (depends on 5)

A method according to claim 5, wherein a first laser beam is aligned perpendicularly to the surface of the mask, is joined by at least one secondary laser beam arranged perpendicularly to the first laser beam, with such joining or admixing taking place via a beam splitter for each secondary laser beam, and with a resulting laser beam being directed onto the joining area.

### Claim 7 (depends on 6)

A method according to claim 6, wherein laser beams either of different wavelengths or of the same wavelength but of different polarisation are used.

### Claim 8 (depends on 5)

A method according to claim 5, wherein several laser beams are focussed parallel to each other onto the joining area by means of a lens.