Methods and apparatus for non-destructive control and forecasting concrete strength
AssigneeThe Concrete Company
InventorsDavid Shtakelberg, Shimon Boyko, Boris Wilge
Life of this patent
Estimating the term…
Abstract
A method of measuring a strength of a capillary-porous chemically active material while hardening, the capillary-porous chemically active material including therein a liquid which undergoes metamorphosis and which is present in the capillary-porous chemically active material in different stages during curing, the method is effected by performing a high frequency, spin-echo nuclear magnetic resonance measurement of each stage of the liquid; and correlating the high frequency, spin-echo nuclear magnetic resonance measurement with a predetermined relationship between the strength and the high frequency, spin-echo nuclear magnetic resonance measurement.
Claims28
A method for measuring a strength of a capillary-porous chemically active material while hardening, the capillary-porous chemically active material including therein water which undergoes stage metamorphosis and including a physically bound water portion having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the material, the method comprising:
- performing a high, at least 7 MHz frequency, spin-echo nuclear magnetic resonance measurement of at least said physically bound water portion;
- and
- correlating said high frequency, spin-echo nuclear magnetic resonance measurement with a predetermined relationship between said strength and said high frequency, spin-echo nuclear magnetic resonance measurement;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
A method for measuring a strength of a capillary-porous chemically active material while hardening, the capillary-porous chemically active material including therein water which undergoes stage metamorphosis and including a physically bound water portion having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the material, the method comprising:
- performing a high, at least 7 MHz frequency, spin-echo nuclear magnetic resonance measurements of at least said physically bound water at least at setting start point and at setting finish point;
- and
- extrapolating said strength based on a predetermined relationship between said strength and said high frequency, spin-echo nuclear magnetic resonance measurements;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
A method of measuring a strength of a structure made of concrete while hardening, the concrete including therein physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the concrete, the method comprising:
- performing an in situ, high at least 7 MHz frequency, spin-echo nuclear magnetic resonance measurement of at least said physically bound water;
- and
- correlating said high frequency, spin-echo nuclear magnetic resonance measurement with a predetermined relationship between said strength and said high MHz frequency, spin-echo nuclear magnetic resonance measurement;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
A method of predicting a strength of a structure made of concrete while hardening, the concrete including therein physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the concrete, the method comprising:
- performing an in situ, a high at least 7 MHz frequency, spin-echo nuclear magnetic resonance measurement of at least said physically bound water;
- and
- extrapolating said strength based on a predetermined relationship between said strength and said high frequency, spin-echo nuclear magnetic resonance measurement;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
An apparatus for measuring a strength of a structure made of a capillary-porous chemically active material while hardening, said capillary-porous chemically active material having a surface and an armature buried in the capillary-porous chemically active material underneath the surface, the capillary-porous chemically active material including therein physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the material, the apparatus comprising a pulsed nuclear magnetic resonance generator for generating a sensitive shallow volume in said concrete structure for performing therein an in situ, high at least 7 MHz frequency, spin-echo nuclear magnetic resonance measurement of at least said physically bound water in the capillary-porous chemically active material while hardening, said pulsed nuclear magnetic resonance generator including in an operative arrangement:
- (a) a static magnetic field generator for generating a static magnetic field within said sensitive volume, said static magnetic field generator including at least one magnet so designed such that static magnetic field lines of said static magnetic field are disposable close and substantially perpendicular to said surface;
- (b) a radio frequency electromagnetic field generator for generating a radio frequency electromagnetic field, said radio frequency electromagnetic field generator including at least one radio frequency coil so designed such that electromagnetic field lines of said radio frequency electromagnetic field are disposable substantially parallel to said surface, so as to avoid interference with the armature being buried in the capillary-porous chemically active material underneath the surface;
- and
- (c) a nuclear magnetic resonance receiver for receiving nuclear magnetic resonance signals form excitable nuclei in said capillary-porous chemically active material and for providing an output indicative of a strength of the capillary-porous chemically active materials.
A method for determining a strength of a capillary-porous chemically active material while hardening, the capillary-porous chemically active material including therein water which undergoes stage metamorphosis and including a portion of physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the material, the method comprising:
- performing a spin-echo nuclear magnetic resonance measurement of at least said physically bound water portion;
- and
- correlating said spin-echo nuclear magnetic resonance measurement with a predetermined relationship between energy values of said physically bound water and said spin-echo nuclear magnetic resonance measurement, thereby determining the strength of the capillary-porous chemically active material while hardening;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
A method for determining a strength of a capillary-porous chemically active material while hardening, the capillary-porous chemically active material including therein water which undergoes stage metamorphosis and including a portion of physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the material, the method comprising:
- performing spin-echo nuclear magnetic resonance measurements of at least said physically bound water at least at setting start point and at setting finish point;
- and
- extrapolating said strength based on a predetermined relationship between said strength and said spin-echo nuclear magnetic resonance measurements;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
A method of determining a strength of a structure made of concrete, the concrete including therein physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the concrete, the method comprising:
- performing an in situ spin-echo nuclear magnetic resonance measurement of at least said physically bound water;
- and
- correlating said spin-echo nuclear magnetic resonance measurement with a predetermined relationship between energy values of said physically bound water and said spin-echo nuclear magnetic resonance measurement, thereby determining the strength of the structure made of concrete while hardening;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
A method of predicting a strength of a structure made of concrete while hardening, the concrete including therein physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the concrete, the method comprising:
- performing an in situ spin-echo nuclear magnetic resonance measurement of at least said physically bound water;
- and
- extrapolating said strength based on a predetermined relationship between said strength and said spin-echo nuclear magnetic resonance measurement;
- wherein, said predetermined relationship is based on:
- (i) linear relation between a quantity of said physically bound water in the material and an amplitude of said spin-echo nuclear magnetic resonance measurement generated by said physically bound water;
- and
- (ii) functional dependency between an energy state of water, as determined by an overall energy of absorption of an RF field, and a relaxation time of water.
An apparatus for measuring a strength of a structure made of a capillary-porous chemically active material, the capillary-porous chemically active material having a surface and an armature buried in the capillary-porous chemically active material underneath the surface, the capillary-porous chemically active material including therein physically bound water having a T2 relaxation time of 30-100 microseconds and a chemically bound water portion having a T2 relaxation time of 10-17 microseconds, the physically bound water portion including water in gel pores and in larger capillaries of the concrete, the apparatus comprising a pulsed nuclear magnetic resonance generator for generating a sensitive volume in said concrete structure for performing therein an in situ, spin-echo nuclear magnetic resonance measurement of at least said physically bound water in the capillary-porous chemically active material while hardening, said pulsed nuclear magnetic resonance generator including in an operative arrangement:
- (a) a static magnetic field generator for generating a static magnetic field within said sensitive volume, said static magnetic field generator including at least one magnet so designed such that static magnetic field lines of said static magnetic field are disposable close and substantially perpendicular to said surface;
- (b) a radio frequency electromagnetic field generator for generating a radio frequency electromagnetic field, said radio frequency electromagnetic field generator including at least one radio frequency coil so designed such that electromagnetic field lines of said radio frequency electromagnetic field are disposable substantially parallel to said surface, so as to avoid interference with the armature being buried in the capillary-porous chemically active material underneath the surface;
- and
- (c) a nuclear magnetic resonance receiver for receiving nuclear magnetic resonance signals form excitable nuclei in said capillary-porous chemically active material and for providing an output indicative of a strength of the capillary-porous chemically active materials.
Dependencies are inferred from the claim text.