# US 6,333,217 B1 · Method of forming MOSFET with channel, extension and pocket implants

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,333,217 B1
- Document ID: US6333217B1
- Status: Granted
- Kind: B1
- Application number: 09/570,391
- Filed: 2000-05-12
- Granted: 2001-12-25
- Earliest claimed: 1999-05-14
- Assignees: Matsushita Electric Industrial Co., Ltd.
- Inventors: Hiroyuki Umimoto; Shinji Odanaka
- Web page: https://patentgrep.com/patent/US6333217B1

## CPC

- H10P 30/21: {of electrically active species}
- H10D 30/0218: {having pocket halo regions selectively formed at the sides of the gates}
- H10D 30/022: {having lightly-doped source or drain extensions selectively formed at the sides of the gates}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 62/371: {Inactive supplementary semiconductor regions, e.g. for preventing punch-through, improving capacity effect or leakage current}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A gate electrode is formed on a semiconductor substrate with a gate insulating film interposed therebetween. A channel region composed of a first-conductivity-type semiconductor layer is formed in a region of a surface portion of the semiconductor substrate located below the gate electrode. Source/drain regions each composed of a second-conductivity-type impurity layer are formed in regions of the surface portion of the semiconductor substrate located on both sides of the gate electrode. Second-conductivity-type extension regions are formed between the channel region and respective upper portion of the source/drain regions in contact relation with the source/drain regions. First-conductivity-type pocket regions are formed between the channel region and respective lower portion of the source/drain regions in contact relation with the source/drain regions and in spaced relation to the gate insulating film.

## Claims

### Claim 1

A method of fabricating a semiconductor device, the method comprising the steps of:
ion implanting a first-conductivity-type impurity into a surface portion of a semiconductor substrate to form a first-conductivity-type semiconductor layer as a channel region;
forming a gate electrode on the semiconductor substrate with a gate insulating film interposed therebetween;
ion implanting a second-conductivity-type impurity into the semiconductor layer by using the gate electrode as a mask to form first second-conductivity-type impurity layers in upper portions of the semiconductor layer;
implanting indium ions into the semiconductor layer by using the gate electrode as a mask to form first-conductivity-type impurity layers in lower portions of the semiconductor layer;
performing a short-time heat treatment with respect to the semiconductor substrate at a temperature of about 950° C. to 1050° C.;
forming sidewalls on side surfaces of the gate electrode; and
ion implanting a second-conductivity-type impurity into the first second-conductivity-type impurity layers and into the first-conductivity-type impurity layers by using the gate electrode and the sidewalls as a mask to form source/drain regions each composed of a second second-conductivity-type impurity layer in respective regions of the first second-conductivity-type impurity layers and the first-conductivity-type impurity layers located on both sides of the gate electrode, form second-conductivity-type extension regions inwardly of respective upper portions of the source/drain regions in the respective first second-conductivity-type impurity layers, and form first-conductivity-type pocket regions inwardly of respective lower portions of the source/drain regions in the respective first-conductivity-type impurity layers.

### Claim 2 (depends on 1)

The method of claim 1, wherein a dose of the indium ions in the step of forming the first-conductivity-type impurity layers is 5×1013 cm−2 or less.

### Claim 3

A method of fabricating a semiconductor device, the method comprising the steps of:
ion implanting a first-conductivity-type impurity into a surface portion of a semiconductor substrate to form a first-conductivity-type semiconductor layer as a channel region;
forming a gate electrode on the semiconductor substrate with a gate insulating film interposed therebetween;
ion implanting an atom belonging to the Group IV into the semiconductor layer by using the gate electrode as a mask to form first-conductivity-type amorphous layers in upper portions of the semiconductor layer;
ion implanting a second-conductivity-type impurity into the amorphous layers by using the gate electrode as a mask to form first second-conductivity-type impurity layers in the respective amorphous layers;
implanting indium ions into the semiconductor layer by using the gate electrode as a mask to form first-conductivity-type impurity layers in lower portions of the semiconductor layer;
performing a short-time heat treatment at a temperature of about 950° C. to 1050° C. with respect to the semiconductor substrate;
forming sidewalls on side surfaces of the gate electrode;
ion implanting a second-conductivity-type impurity into the first second-conductivity-type impurity layers and into the first-conductivity-type impurity layers by using the gate electrode and the sidewalls as a mask to form source/drain regions each composed of a second second-conductivity-type impurity layer in respective regions of the first second-conductivity-type impurity layers and the first-conductivity-type impurity layers located on both sides of the gate electrode, form second-conductivity-type extension regions inwardly of respective upper portions of the source/drain regions in the respective first second-conductivity-type impurity layers, and form first-conductivity-type pocket regions inwardly of respective lower portions of the source/drain regions in the respective first-conductivity-type impurity layers.

### Claim 4 (depends on 3)

The method of claim 3, wherein a dose of the indium ions in the step of forming the first-conductivity-type impurity layers is 5×1013 cm−2 or less.

### Claim 5

A method of fabricating a semiconductor device, the method comprising the steps of:
implanting indium ions into a surface portion of a semiconductor substrate to form a first-conductivity-type semiconductor layer as a channel region;
forming a gate electrode on the semiconductor substrate with a gate insulating film interposed therebetween;
ion implanting a second-conductivity-type impurity into the semiconductor layer by using the gate electrode as a mask to form first second-conductivity-type impurity layers in upper portions of the semiconductor layer;
depositing an insulating film over the entire surface of the semiconductor substrate at a temperature of about 600° C. to 850° C. to form first-conductivity-type lightly doped channel regions inwardly of the respective first second-conductivity-type impurity layers and in upper portions of the semiconductor layer, each of the lightly doped channel regions containing the impurity at a concentration lower than in the semiconductor layer;
performing anisotropic etching with respect to the insulating film to form sidewalls on side surfaces of the gate electrode; and
ion implanting a second-conductivity-type impurity into the first second-conductivity-type impurity layers and into the semiconductor layer by using the gate electrode and the sidewalls as a mask to form source/drain regions each composed of a second second-conductivity-type impurity layer in respective regions of the first second-conductivity-type impurity layers and the semiconductor layer located on both sides of the gate electrode and form second-conductivity-type extension regions inwardly of respective upper portions of the source/drain regions in the respective first second-conductivity-type impurity layers.

### Claim 6

A method of fabricating a semiconductor device, the method comprising the steps of:
forming a first-conductivity-type semiconductor layer as a channel region by implanting indium ions into a surface portion of a semiconductor substrate;
forming a gate electrode on the semiconductor substrate with a gate insulating film interposed therebetween;
ion implanting an atom belonging to the Group IV by using the gate electrode as a mask to form first-conductivity-type amorphous layers in upper portions of the semiconductor layer;
ion implanting a second-conductivity-type impurity into the amorphous layers by using the gate electrode as a mask to form first second-conductivity-type impurity layers;
depositing an insulating film over the entire surface of the semiconductor substrate at a temperature of about 600° C. to 850° C. to form first-conductivity-type lightly doped channel regions inwardly of the respective first second-conductivity-type impurity layers and in upper portions of the semiconductor layer, each of the lightly doped channel regions containing the impurity at a concentration lower than in the semiconductor layer;
performing anisotropic etching with respect to the insulating film to form sidewalls on side surfaces of the gate electrode; and
ion implanting a second-conductivity-type impurity into the first second-conductivity-type impurity layers and into the semiconductor layer by using the gate electrode and the sidewalls as a mask to form source/drain regions each composed of a second second-conductivity-type impurity layer in respective regions of the first second-conductivity-type impurity layers and the semiconductor layer located on both sides of the gate electrode and form second-conductivity-type extension regions inwardly of respective upper portions of the source/drain regions in the respective first second-conductivity-type impurity layers.

### Claim 7

A method of fabricating a semiconductor device, the method comprising the steps of:
implanting indium ions into a surface portion of a semiconductor substrate to form a first-conductivity-type semiconductor layer as a channel region;
forming a gate electrode on the semiconductor substrate with a gate insulating film interposed therebetween;
ion implanting a second-conductivity-type impurity into the semiconductor layer by using the gate electrode as a mask to form first second-conductivity-type impurity layers in upper portions of the semiconductor layer;
performing a long-time first heat treatment with respect to the semiconductor substrate at a temperature of about 600° C. to 850° C. to form first-conductivity-type lightly doped channel regions inwardly of the respective first second-conductivity-type impurity layers and in upper portions of the semiconductor layer, each of the lightly doped channel regions containing the impurity at a concentration lower than in the semiconductor layer;
implanting indium ions into the semiconductor layer by using the gate electrode as a mask to form first-conductivity-type impurity layers in lower portions of the semiconductor layer;
performing a short-time second heat treatment at a temperature of about 950° C. to 1050° C. with respect to the semiconductor substrate;
forming sidewalls on side surfaces of the gate electrode; and
ion implanting a second-conductivity-type impurity into the first second-conductivity-type impurity layers and into the first-conductivity-type impurity layers by using the gate electrode and the sidewalls as a mask to form source/drain regions each composed of a second second-conductivity-type impurity layer in respective regions of the first second-conductivity-type impurity layers and the first-conductivity-type impurity layers located on both sides of the gate electrode, form second-conductivity-type extension regions inwardly of respective upper portions of the source/drain regions in the respective first second-conductivity-type impurity layers, and form second-conductivity-type pocket regions inwardly of respective lower portions of the source/drain regions in the respective second-conductivity-type impurity layers.

### Claim 8

A method of fabricating a semiconductor device, the method comprising the steps of:
ion implanting a first-conductivity-type impurity into a surface portion of a semiconductor substrate to form a first-conductivity-type semiconductor layer as a channel region;
forming a gate electrode on the semiconductor substrate with a gate insulating film interposed therebetween;
ion implanting an atom belonging to the Group IV into the semiconductor layer by using the gate electrode as a mask to form first-conductivity-type amorphous layers in upper regions of the semiconductor layer;
ion implanting a second-conductivity-type impurity into the amorphous layers by using the gate electrode as a mask to form first second-conductivity-type impurity layers in the respective amorphous layers;
depositing an insulatint film over the entire surface of the semiconductor substrate at a temperature of about 600° C. to 850° C. to form first-conductivity-type lightly doped channel regions inwardly of the first second-conductivity-type impurity layers and in upper portions of the semiconductor layer, each of the lightly doped channel regions containing the impurity at a concentration lower than in the semiconductor layer;
performing anisotropic etching with respect to the insulating film to form sidewalls on side surfaces of the gate electrode; and
ion implanting a second-conductivity-type impurity into the first second-conductivity-type impurity layers and into the semiconductor layer by using the gate electrode and the sidewalls as a mask to form source/drain regions each composed of a second second-conductivity-type impurity layer in respective lower portions of the first second-conductivity-type impurity layers and the semiconductor layer located on both sides of the gate electrode and form second-conductivity-type extension regions inwardly of respective upper portions of the source/drain regions in the respective first second-conductivity-type impurity layers; and
after removing the sidewalls, implanting indium ions into the semiconductor layer by using the gate electrode as a mask to form first-conductivity-type pocket regions inwardly of respective lower portions of the source/drain regions and in lower portions of the semiconductor layer.

### Claim 9

A method of fabricating a semiconductor device, the method comprising the steps of:
implanting indium ions into a surface portion of a semiconductor substrate to form a first-conductivity-type semiconductor layer as a channel region;
forming a gate electrode on the semiconductor substrate with a gate insulating film interposed therebetween;
ion implanting an atom belonging to the Group IV by using the gate electrode as a mask to form Group-IV-atom-ion implanted layers in upper portions of the semiconductor layer;
performing a long-time first heat treatment with respect to the semiconductor substrate at a temperature of about 600° C. to 850° C. to form first-conductivity-type lightly doped impurity layers into respective upper portions of the Group-IV-atom-ion implanted layers and the semiconductor layer, each of the lightly doped impurity layers containing the activated impurity at a concentration lower than in the semiconductor layer;
implanting indium ions into the semiconductor layer by using the gate electrode as a mask to form first-conductivity-type impurity layers in lower portions of the semiconductor layer;
ion implanting a second-conductivity-type impurity into the semiconductor layer by using the gate electrode as a mask to form first second-conductivity-type impurity layers in upper portions of the semiconductor layer and form lightly doped channel regions composed of the first-conductivity-type lightly doped impurity layers inwardly of the respective first second-conductivity-type impurity layers;
performing a short-time second heat treatment at a temperature of about 950° C. to 1050° C. with respect to the semiconductor substrate;
forming sidewalls on side surfaces of the gate electrode; and
ion implanting a second-conductivity-type impurity into the first second-conductivity-type impurity layers and into the first-conductivity-type impurity layers by using the gate electrode and the sidewalls as a mask to form source/drain regions each composed of a second second-conductivity-type impurity layer in respective regions of the first second-conductivity-type impurity layers and the first-conductivity-type impurity layers located on both sides of the gate electrode, form second-conductivity-type extension regions inwardly of respective upper portions of the source/drain regions in the respective first second-conductivity-type impurity layers, and form first-conductivity-type pocket regions inwardly of respective lower portions of the source/drain regions in the respective first-conductivity-type impurity layers.