Rosin/hydrocarbon resin size for paper
AssigneeHercules Incorporated
InventorsSusan M. Ehrhardt, D. Bruce Evans
Life of this patent
Estimating the term…
Loading patent…
AssigneeHercules Incorporated
InventorsSusan M. Ehrhardt, D. Bruce Evans
Estimating the term…
Discloses is a method for sizing paper at a pH of about 5.0 to about 8.5 by incorporating a sizing composition consisting essentially of (a) rosin, (b) at least one hydrocarbon resin, (c) a cationic component consisting essentially of a cationic polyamine resin at a weight ration of the rosin/hydrocarbon resin blend to cationic polyamine of about 5:1 to about 1:2, and (d) up to 0.3% alum. The cationic polyamine resin is selected from the group consisting of polyalkyleneamine-epihalohydrin resins, polyalkyleneamine-dicyandiamide-epihalohydrin resins, poly(diallylamine•HCl)-epihalohydrin resins, poly(methyldiallylamine•HCl)-epihalohydrin resins, epihalohydrin-modified polyethyleneimine resins, amine-modified poly(methyldiallylamine•HCl)-epihalohydrin resins, and mixtures thereof.
A method for sizing paper or paperboard, said method consisting essentially of incorporating into the paper or paperboard pulp at a pH of about 5.0 to about 8.5 a sizing composition consisting essentially of (a) about 0.1 to about 1% by weight of rosin, based upon the dry weight of the pulp, (b) about 10 to about 90% of at least one hydrocarbon resin, based upon the total weight of the rosin and hydrocarbon resin, (c) a cationic component consisting essentially of a cationic polyamine resin, wherein the weight ratio of the rosin and hydrocarbon resin to cationic resin is about 5:1 to about 1:2 and the cationic polyamine resin is selected from the group consisting of polyalkyleneamine-epihalohydrin resins, polyalkyleneamine-dicyandiamide-epihalohydrin resins, poly(diallylamine•HCl)-epihalohydrin resins, poly(methyldiallylamine•HCl)-epihalohydrin resins, epihalohydrin-modified polyethyleneimine resins, amine-modified poly(methyldiallylamine•HCl)-epihalohydrin resins, and mixtures thereof, and (d) up to 0.3% alum, based on the dry weight of the pulp.
A method for sizing paper or paperboard said method consisting essentially of incorporating into the paper or paperboard pulp at a pH of about 5.0 to about 8.5 a sizing composition consisting essentially of (a) about 0.1 to about 1% by weight of rosin, based upon the dry weight of the pulp, (b) about 10 to about 90% of at least one hydrocarbon resin, based upon the total weight of the rosin and hydrocarbon resin, (c) a cationic component consisting essentially of a cationic polyamine resin, wherein the weight ratio of the rosin and hydrocarbon resin to cationic resin is about 5:1 to about 1:2 and the cationic polyamine resin is selected from the group consisting of polyalkyleneamine-epihalohydrin resins, polyalkyleneamine-dicyandiamide-epihalohydrin resins, poly(diallylamine•HCl)-epihalohydrin resins, poly(methyldiallylamine•HCl)-epihalohydrin resins, epihalohydrin-modified polyethyleneimine resins, amine-modified poly(methyldiallylamine•HCl)-epihalohydrin resins, and mixtures thereof, and (d) up to 0.1% alum, based on the dry weight of the pulp.
A method for anchoring a rosin-based size to paper pulp, said method consisting essentially of incorporating into the paper or paperboard pulp at a pH of about 5.0 to about 8.5 a sizing composition consisting essentially of (a) about 0.1 to about 1% by weight of rosin, based upon the dry weight of the pulp, (b) about 10 to about 90% of at least one hydrocarbon resin, based upon the total weight of the rosin and hydrocarbon resin, (c) a cationic component consisting essentially of a cationic polyamine resin, wherein the weight ratio of the rosin and hydrocarbon resin to cationic resin is about 5:1 to about 1:2 and the cationic polyamine resin is selected from the group consisting of polyalkyleneamine-epihalohydrin resins, polyalkyleneamine-dicyandiamide-epihalohydrin resins, poly(diallylamine•HCl)-epihalohydrin resins, poly(methyldiallylamine•HCl)-epihalohydrin resins, epihalohydrin-modified polyethyleneimine resins, amine-modified poly(methyldiallylamine•HCl)-epihalohydrin resins, and mixtures thereof, and (d) up to 0.3% alum, based on the dry weight of the pulp.
A method for anchoring a rosin-based size to paper pulp, said method consisting essentially of incorporating into the paper or paperboard pulp at a pH of about 5.0 to about 8.5 a sizing composition consisting essentially of (a) about 0.1 to about 1% by weight of rosin, based upon the dry weight of the pulp, (b) about 10 to about 90% of at least one hydrocarbon resin, based upon the total weight of the rosin and hydrocarbon resin, (c) a cationic component consisting essentially of a cationic polyamine resin, wherein the weight ratio of the rosin and hydrocarbon resin to cationic resin is about 5:1 to about 1:2 and the cationic polyamine resin is selected from the group consisting of polyalkyleneamine-epihalohydrin resins, polyalkyleneamine-dicyandiamide-epihalohydrin resins, poly(diallylamine•HCl)-epihalohydrin resins, poly(methyldiallylamine•HCl)-epihalohydrin resins, epihalohydrin-modified polyethyleneimine resins, amine-modified poly(methyldiallylamine•HCl)-epihalohydrin resins, and mixtures thereof, and (d) up to 0.1% alum, based on the dry weight of the pulp.
Dependencies are inferred from the claim text.