US 6,273,921 B1Granted
Battery fabrication method using supercritical carbon dioxide
AssigneeThe Boeing Company
InventorsThomas B. Stanford, John D. Margerum, Willis H. Smith, Jr.
Life of this patent
Estimating the term…
Abstract
A method for making batteries wherein the extraction step includes extracting plasticizer using phase shifting of supercritical carbon dioxide. In addition, contacting the extracting cells with pressurized carbon dioxide throughout the fabrication process encourages the formation of a solid electrolyte interphase layer.
Claims8
A method of making a battery comprising:
- forming one or more cells containing plasticizer;
- securing said one or more cells in an airtight leak-free extraction chamber, said chamber in fluid communication with a fluid delivery system;
- contacting the cells with a compressed or dense phase gas consisting essentially of carbon dioxide, said carbon dioxide at a pressure and temperature equal to, above, or below the critical pressure and/or critical temperature of carbon dioxide;
- extracting the cell(s) maintained at a temperature above the critical temperature of carbon dioxide by sequentially flowing compressed or dense phase carbon dioxide extraction solvent and then changing the phase of the carbon dioxide between the supercritical state and the liquid state by varying the pressure of the carbon dioxide in a series of alternating steps between two pressures at or above the critical pressure of carbon dioxide, maintaining said pressure at the completion of each step for a period of time sufficient to remove the plasticizer and/or one or more contaminants, said maintaining contact between said carbon dioxide and said one or more cells for said period of time at each step;
- changing the phase of the carbon dioxide without attempting to minimize or modulate any change in the temperature of the fluid during the phase change;
- varying the temperature of the carbon dioxide by causing a rapid and significant change in pressure of the fluid by either expansion to produce cooling or compression to produce heating of the fluid;
- contacting said one or more cells with an electrolyte;
- applying 15-20 pounds per square inch of static carbon dioxide pressure to said extraction chamber;
- applying and then releasing a static pressure plug of 20-100 pounds per square inch of carbon dioxide pressure to the extraction chamber to remove an excess of said electrolyte;
- and
- applying 15-20 pounds per square inch of static carbon dioxide pressure to said extraction chamber.
8 more elements
A method of making a battery comprising:
- forming one or more cells containing plasticizer;
- securing said one or more cells in an airtight leak-free extraction chamber, said chamber in fluid communication with a fluid delivery system;
- contacting the cells with a compressed or dense phase gas consisting essentially of carbon dioxide, said carbon dioxide at a pressure and temperature equal to, above, or below the critical pressure and/or critical temperature of carbon dioxide;
- extracting the cell(s) by sequentially flowing compressed or dense phase carbon dioxide extraction solvent and then changing the phase of the carbon dioxide between the liquid state and the supercritical state by varying the temperature of the carbon dioxide in a series of steps between a temperature at above the critical temperature of carbon dioxide and a temperature below the critical temperature of carbon dioxide, maintaining said temperature at the completion of each step for a period of time sufficient to remove the plasticizer and/or one or more contaminants, said maintaining contact between said carbon dioxide and said one or more cells for said period of time at each step;
- changing the phase of the carbon dioxide without attempting to minimize or modulate any change in the pressure of the fluid during the phase change;
- varying the temperature of the carbon dioxide by causing a rapid and significant change in pressure of the fluid by either expansion to produce cooling or compression to produce heating of the fluid;
- contacting said one or more cells with an electrolyte;
- applying 15-20 pounds per square inch of static carbon dioxide pressure to said extraction chamber;
- applying and then releasing a static pressure plug of 20-100 pounds per square inch of carbon dioxide pressure to the extraction chamber to remove an excess of said electrolyte;
- and
- applying 15-20 pounds per square inch of static carbon dioxide pressure to said extraction chamber.
8 more elements
Dependencies are inferred from the claim text.