Fine-grained WC-Co cemented carbide
AssigneeSandvik AB
InventorRolf Oskarsson
Life of this patent
Estimating the term…
Abstract
The present invention relates to a method of making a WC—Co-based cemented carbide with a sintered mean WC-grain size in the range 0.4-1.6 μm. the cemented carbide is produced from well deagglomerated or easy to deagglomerate WC powder with round morphology, a Co powder also well deagglomerated or easy to deagglomerate and with a grain size equal to or smaller than the WC grain size and grain growth inhibitors. According to the invention the metal part of the grain growth inhibitors is added as part of the binder phase i.e., is included in the Co powder and alloyed therewith.
Claims8
A method of making a WC—Co-based cemented carbide with a sintered mean WC-grain size in the range 0.4-1.6 μm, wherein the method comprises the steps of:
- (a) providing a WC powder with a round morphology;
- (b) providing a Co powder alloyed with at least one grain growth inhibitor;
- and
- (c) mixing the WC powder and the Co powder.