Absorbent article and production process therefor
AssigneeNippon Shokubai Co., Ltd.
InventorsKatsuyuki Wada, Naoko Takahashi, Hiroko Ueda, Kinya Nagasuna
Life of this patent
Estimating the term…
Loading patent…
AssigneeNippon Shokubai Co., Ltd.
InventorsKatsuyuki Wada, Naoko Takahashi, Hiroko Ueda, Kinya Nagasuna
Estimating the term…
The invention clarifies absorption properties of a water-absorbent resin as needed in the case where the ratio by weight of the water-absorbent resin to the total of the water-absorbent resin and the fibrous material is ".alpha.," and further the invention provides an absorbent article using a water-absorbent resin which is optimal to the ratio by weight ".alpha." of the water-absorbent resin. A water-absorbent resin, having a concentration absorption index of 35 or more as shown by the following equation (1): A(1-.alpha.)+B.alpha. (1) wherein A (g/g) is an absorption capacity of the resin under no load, and B (g/g) is an absorption capacity of the resin under a load, is used as the water-absorbent resin as used for the absorbent article of at least 0.4 in the ratio by weight ".alpha." of the water-absorbent resin to the total of the water-absorbent resin and the fibrous material.
A process for producing an absorbent article having an absorbent layer, a liquid-permeable surface sheet, and a liquid-impermeable back sheet, wherein the absorbent layer includes an absorbent matter having a water-absorbent resin and a fibrous material in a ratio by weight, ".alpha.," of the water-absorbent resin to the total of the water-absorbent resin and the fibrous material, wherein the ratio by weight ".alpha." is at least 0.4, with the process comprising the step of using as the water-absorbent resin a water-absorbent resin which has a concentration absorption index of 35 or more as shown by the following equation (1):
An absorbent article, comprising an absorbent layer, a liquid-permeable surface sheet, and a liquid-impermeable back sheet, wherein the absorbent layer includes an absorbent matter having a water-absorbent resin and a fibrous material in a ratio by weight, ".alpha.," of the water-absorbent resin to the total of the water-absorbent resin and the fibrous material, wherein the ratio by weight ".alpha." is at least 0.4, and wherein the water-absorbent resin has a concentration absorption index of 35 or more as shown by the following equation (1):
Dependencies are inferred from the claim text.