Laminate sheet and tent made therefrom
AssigneeTeijin Limited
InventorsNoritugu Saiki, Hodaka Yokomizo
Life of this patent
Estimating the term…
Abstract
A laminate sheet comprising (A) a polyester block copolymer which comprises 20 to 70 wt % of a hard segment consisting of an aromatic polyester and 80 to 30 wt % of a soft segment consisting of an aromatic polyester and (B) cloth on at least one side of which the polyester block copolymer is laminated, the melting point (T,.degree. C.) of the polyester block copolymer satisfying the following expressions: T0-5 >T>T0-60 and T>T'+10 (in which T is defined above, T0 is a melting point (0.degree. C.) of the aromatic polyester constituting the hard segment, and T' is a melting point (.degree. C.) of a random polymer obtained by adding 0.1 wt % of titanium tetrabutoxide to the polyester block copolymer and melting and kneading at 250.degree. C. for 3 hours).
Claims21
A laminate sheet comprising:
- (A) a polyester block copolymer which comprises 20 to 70 wt % of a hard segment consisting of an aromatic polyester comprising terephthalic acid in an amount of at least 60 mol % of the total of all dicarboxylic acid components and tetramethylene glycol in an amount of at least 60 mol % of the total of all diol components, and 80 to 30 wt % of a soft segment consisting of an aromatic polyester comprising at least one diol selected from the group consisting of diols represented by the following formula (1):
- ##STR4## wherein n is a number of 2 to 5, and aliphatic diols represented by the following formula (2):
- ##STR5## wherein m is a number of 5 to 12, and R is a hydrogen atom or a methyl group, provided that a plurality of R's may be the same or different,
- in an amount of at least 60 mol % of the total of all diol components and an aromatic dicarboxylic acid in an amount of at least 60 mol % of the total of all dicarboxylic acid components,
- the melting point (T,.degree. C.) of the polyester block copolymer satisfying the following expressions (3) and (4):
- T0-5 >T>T0-60 (3)
- T>T'+10 (4)
- wherein T is defined above, T0 is a melting point (.degree. C.) of the aromatic polyester constituting the hard segment, and T' is a melting point (.degree. C.) of a random polymer obtained by adding 0.1 wt % of titanium tetrabutoxide to the polyester block copolymer and melting and kneading at 250.degree. C. for 3 hours;
- and
- (B) cloth on at least one side of which the polyester block copolymer is laminated.