# US 6,146,552 A · Zinc oxide ceramics and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,146,552 A
- Document ID: US6146552A
- Status: Granted
- Kind: A
- Application number: 09/022,609
- Filed: 1998-02-12
- Granted: 2000-11-14
- Earliest claimed: 1995-03-06
- Assignees: Matsushita Electric Industrial Co., Ltd.
- Inventors: Atsushi Iga; Hideyuki Okinaka; Masahiro Ito
- Web page: https://patentgrep.com/patent/US6146552A

## CPC

- H01C 7/112: ZnO type
- C04B 35/453: based on zinc, tin, or bismuth oxides or solid solutions thereof with other oxides, e.g. zincates, stannates or bismuthates
- H01C: RESISTORS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Zinc oxide ceramics and a method for producing the same are provided wherein zinc oxide varistors for low and high voltages having excellent electric characteristics and high reliability upon DC loading and surge can be obtained in high yield by low-temperature sintering. 0.2 to 20 parts by weight of a mixed powder of bismuth oxide, titanium oxide and antimony oxide is treated in advance at a temperature of 850.degree. C. or less. The synthetic powder thus obtained is added to 100 parts by weight of ZnO material powder to produce ceramics. By using the ceramics for a zinc oxide varistor, a zinc oxide varistor for a low or high voltage can be produced in high yield, which can be sintered at a low temperature and is excellent in electric characteristics and reliability upon DC loading and surge. Aluminum is sprayed on both sides of a sintered body so that an aluminum layer is formed. Copper is sprayed on the aluminum layer so that an electrode is formed. A lead wire is bonded to the electrode. Then, portions of the molded bodies other than the lead wire are coated and insulated so that the zinc oxide varistor can be obtained.

## Claims

### Claim 1

A zinc oxide ceramic comprising a sintered mixture of a first component, a second component and a third component that comprises:
100 parts by weight of zinc oxide as the first component:
0.1 to 5.0 parts by weight of at least one of cobalt oxide and manganese oxide as the second component; and
0.2 to 20 parts by weight of a powder mixture of the oxides of bismuth, titanium and antimony as the third component;
wherein the third component is heated at temperatures of 450.degree. C. to 800.degree. C. before a mixture of the first, second and third components is formed, and
wherein the ceramic is suitable for use with an Ag electrode.

### Claim 2 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the third component further comprises at least one selected from boron oxide and boric acid.

### Claim 3 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the third component further comprises chromium oxide.

### Claim 4 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the amount of bismuth oxide is 0.3 to 10.0 parts by weight for 100 parts by weight of zinc oxide by Bi.sub.2 O.sub.3 conversion.

### Claim 5 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the amount of titanium oxide is 0.1 to 5.0 parts by weight for 100 parts by weight of zinc oxide by TiO.sub.2 conversion.

### Claim 6 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the amount of antimony oxide is 0.02 to 2.5 parts by weight for 100 parts by weight of zinc oxide by Sb.sub.2 O.sub.3 conversion.

### Claim 7 (depends on 2)

The zinc oxide ceramic according to claim 2, wherein the boron oxide is boron trioxide.

### Claim 8 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the first component contains 0.00062 to 0.372 part by weight of an aluminum component for 100 parts by weight of zinc oxide by Al.sub.2 O.sub.3 conversion.

### Claim 9 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the third component comprises a synthetic powder prepared by heat treating a mixture of bismuth oxide and boron oxide that is added to a synthetic powder prepared by heat-treating a mixed powder of at least bismuth oxide, titanium oxide and antimony oxide.

### Claim 10 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the third component comprises a synthetic powder prepared by heat treating a mixture of bismuth oxide and chromium oxide that is added to a synthetic powder prepared by heating treating a mixed powder of at least bismuth oxide, titanium oxide and antimony oxide.

### Claim 11 (depends on 1)

The zinc oxide ceramic according to claim 1, wherein the third component comprises a synthetic powder prepared by heat treating a mixture of bismuth oxide and chromium oxide and a synthetic powder prepared by heat-treating a mixture of bismuth oxide and boron oxide that are added to a synthetic powder prepared by heat treating a mixed powder of at least titanium oxide and antimony oxide.

### Claim 12 (depends on 1)

A zinc oxide varistor, comprising a zinc oxide ceramic according to claim 1 and an Ag electrode.

### Claim 13

A zinc oxide ceramic comprising a sintered mixture of a first component, a second component and a third component that comprises:
100 parts by weight of zinc oxide as the first component;
0.1 to 5.0 parts by weight of at least one of cobalt oxide and manganese oxide as the second component; and
0.5 to 20 parts by weight of a powder mixture of the oxides of bismuth, titanium, antimony, and chromium, and at least one of boron oxide and boric acid, as the third component;
wherein the third component is heated at temperatures of 450.degree. C. to 800.degree. C. before a mixture of the first, second and third components is formed, and
wherein the ceramic is suitable for use with an Ag electrode.

### Claim 14 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the average particle size of the third component is 0.05 to 10 .mu.m.

### Claim 15 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the manganese oxide is at least one of MnO, Mn.sub.2 O.sub.3 and MnO.sub.2.

### Claim 16 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the cobalt oxide is at least one of CoO and Co.sub.3 O.sub.4.

### Claim 17 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the amount of bismuth oxide is 0.3 to 18.0 parts by weight for 100 parts by weight of zinc oxide by Bi.sub.2 O.sub.3 conversion.

### Claim 18 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the amount of titanium oxide is 0.03 to 2.00 parts by weight for 100 parts by weight of zinc oxide by TiO.sub.2 conversion.

### Claim 19 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the amount of antimony oxide is 0.005 to 1.000 part by weight for 100 parts by weight of zinc oxide by Sb.sub.2 O.sub.3 conversion.

### Claim 20 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the amount of chromium oxide is 0.005 to 0.500 part by weight for 100 parts by weight of zinc oxide by Cr.sub.2 O.sub.3 conversion.

### Claim 21 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the amount of boron oxide is 0.002 to 1.000 part by weight for 100 parts by weight of zinc oxide by B.sub.2 O.sub.3 conversion.

### Claim 22 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the boron oxide is B.sub.2 O.sub.3.

### Claim 23 (depends on 13)

The zinc oxide ceramic according to claim 13, wherein the first component comprises 0.00062 to 0.37200 part by weight of an aluminum oxide for 100 parts by weight of zinc oxide by Al.sub.2 O.sub.3 conversion.

### Claim 24 (depends on 13)

A zinc oxide varistor, comprising a zinc oxide ceramic according to claim 13 and an Ag electrode.