Plain bearing
AssigneeFederal-Mogul Wiesbaden GmbH
InventorsGerd Andler, Jens-Peter Heinss, Klaus Goedicke, Christoph Metzner
Life of this patent
Estimating the term…
Loading patent…
AssigneeFederal-Mogul Wiesbaden GmbH
InventorsGerd Andler, Jens-Peter Heinss, Klaus Goedicke, Christoph Metzner
Estimating the term…
A plain bearing is described, the overlay (3) of which exhibits properties which are markedly improved with regard to wear resistance in comparison with overlays applied by electroplating and conventional electron beam vapor deposition methods. The surface of the overlay (3) comprises round raised portions (4) and depressed portions (6), wherein, in relation to the horizontal section plane (7), the raised portions (4) cover a proportion of the surface area amounting to 30% to 50%, based on the entire surface area of the plain bearing, the section plane (7) being at a height at which the total proportion of the surface area consisting of the raised portions (4), and obtained in vertical section, is equal to the total corresponding proportion consisting of the depressed portions (6). The round raised portions exhibit a diameter D of 3 to 8 .mu.m, in plan view, wherein, in the case of raised portions (4) and depressed portions (6) which in plan view are not circular, this value relates to the maximum diameter. The surface exhibits a roughness of R.sub.z =3 to 7 .mu.m. The method of producing such plain bearings is based on electron beam vapour deposition, wherein a backing member with a roughness of R.sub.z .ltoreq.2 .mu.m is used and vapor deposition of the overlay is effected at a pressure <0.1 Pa.
A plain bearing comprising a backing member and at least one metallic overlay, which is applied by electron beam vapour deposition, characterised in that
Dependencies are inferred from the claim text.