Process for making a detergent composition by non-tower process
AssigneeThe Procter & Gamble Company
InventorsAngela Gloria Del Greco, Wayne Edward Beimesch
Life of this patent
Estimating the term…
Abstract
A non-tower process for continuously preparing granular detergent composition having a density of at least about 600 g/l is provided. The process comprises the steps of (a) dispersing a surfactant and coating the surfactant with fine powder having a diameter from 0.1 to 500 microns in a mixer fitted with choppers, and (b) granulating the agglomerates in one or more fluidizing apparatus, wherein finely atomized liquid is sprayed onto the first agglomerates in a mixer between step (a) and (b).
Claims8
A non-tower process for preparing a granular detergent composition having a density of at least about 600 g/l, consisting of the steps of:
- (a) dispersing a surfactant, and coating the surfactant with fine powder having a diameter from 0.1 to 500 microns, in a mixer fitted with choppers wherein conditions of the mixer include (i) from about 0.5 to about 15 minutes of mean residence time and (ii) from about 0.15 to about 7 kj/kg of energy condition, wherein first agglomerates are formed;
- (a') spraying finely atomized liquid onto the first agglomerates in a mixer wherein conditions of the mixer include (i) from about 0.2 to about 5 seconds of mean residence time, (ii) from about 10 to about 30 m/s of tip speed, and (iii) from about 0.15 to about 5 kj/kg of energy condition, wherein second agglomerates are formed;
- (b) granulating the second agglomerates in one or more fluidizing apparatus wherein conditions of each of the fluidizing apparatus include (i) from about 1 to about 10 minutes of mean residence time, (ii) from about 100 to about 300 mm of depth of unfluidized bed, (iii) not more than about 50 micron of droplet spray size, (iv) from about 175 to about 250 mm of spray height, (v) from about 0.2 to about 1.4 m/s of fluidizing velocity and (vi) from about 12 to about 100.degree. C. of bed temperature;
- (c) optionally dispersing an aqueous or non-aqueous polymer solution with said surfactant is step (a);
- (d) optionally adding an internal recycle stream of powder from the fluidizing apparatus to step (a);
- and
- (e) optionally adding excessive fine powder further formed in step (a) into step (a').
Dependencies are inferred from the claim text.