# US 6,096,495 A · Method for preparing silver halide emulsion

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,096,495 A
- Document ID: US6096495A
- Status: Granted
- Kind: A
- Application number: 09/113,935
- Filed: 1998-07-10
- Granted: 2000-08-01
- Earliest claimed: 1997-07-15
- Assignees: Konica Corporation
- Inventors: Shigetami Kasai; Hisatake Okada
- Web page: https://patentgrep.com/patent/US6096495A

## CPC

- B01F 25/23: Mixing by intersecting jets
- G03C 1/0051: {Tabular grain emulsions}
- G03C 1/015: Apparatus or processes for the preparation of emulsions (coating, drying G03C1/74 {; G03C1/07 takes precedence; special processes for tabular grains G03C1/0051})
- B01F 23/41: Emulsifying
- B01F 2025/9122: {from the circumference to the center}
- G03C 2001/0055: {Aspect ratio of tabular grains in general; High aspect ratio; Intermediate aspect ratio; Low aspect ratio}
- G03C 2001/03529: {Coefficient of variation}
- G03C 2001/0357: {Monodisperse emulsion}
- G03C 2001/03594: {Size of the grains}
- G03C 2200/09: Apparatus
- G03C 2200/43: Process
- B01F: MIXING, e.g. DISSOLVING, EMULSIFYING OR DISPERSING (mixing paints B44D3/06)
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

A method for preparing a silver halide emulsion is disclosed, comprising introducing a silver salt solution and a halide solution through separate introduction tubes, mixing the silver salt and halide solutions to react a silver salt and a halide to form silver halide grains and discharging a reaction mixture solution through a discharge tube by the use of a mixing apparatus in which the introduction tubes and the discharge conduit are linked together so that all center axes of the introduction and discharge tubes intersect at a single point, wherein the silver salt solution and the halide solution are independently introduced at a linear velocity of not less than 4.0 m/sec and a Reynolds number of not less than 3,000.

## Claims

### Claim 1

A method for preparing a silver halide emulsion, comprising:
introducing a silver salt solution and a halide solution through separate introduction tubes, said silver salt solution containing a maximum of 0.01 mol per liter of a silver salt,
mixing the silver salt and halide solutions to react a silver salt and a halide to form silver halide grains,
discharging a reaction mixture solution through a discharge conduit and
using a mixing apparatus in which the introduction tubes and the discharge conduit are linked together so that all center axes of the introduction tubes and discharge conduit intersect at a single point,
wherein the silver salt solution and the halide solution are independently introduced at a linear velocity of not less than 4.0 m/sec and a Reynolds number of not less than 3,000.

### Claim 2 (depends on 1)

The method of claim 1, wherein the Reynolds number is not less than 10,000.

### Claim 3 (depends on 1)

The method of claim 1, wherein the linear velocity is not less than 5.0 m/sec.

### Claim 4 (depends on 1)

The method claim 1, wherein the silver salt solution and the halide solution are independently introduced at a linear velocity of not less than 10.0 m/sec and the reaction mixture solution is discharged at a linear velocity of not less than 20 m/sec.

### Claim 5 (depends on 1)

The method of claim 1, wherein a difference in an inner diameter between the introduction tubes is not more than 10%.

### Claim 6 (depends on 1)

The method of claim 1, wherein a difference in an inner diameter between the introduction tubes and the discharge conduit is not more than 10%.

### Claim 7 (depends on 1)

The method of claim 1, wherein a difference in a molar concentration between the silver salt solution and the halide solution is not more than 10%.

### Claim 8 (depends on 1)

The method of claim 1, wherein the silver salt solution and the halide solution are each introduced through the introduction tubes by the use of a pump having a pulsating flow within .+-.2% of the average flow rate.

### Claim 9 (depends on 1)

The method of claim 1, wherein the silver halide grains formed have an average grain size of not more than 0.05 .mu.m and a variation coefficient of grain size of not more than 20%, and at least 50% of the total number of the silver halide grains formed being accounted for by tabular grains having two parallel twin planes.

### Claim 10 (depends on 1)

The method of claim 1, wherein the silver halide grains formed are discharged through the discharge conduit and then introduced into a reaction vessel to allow the silver halide grains to grow therein, and wherein the silver potential in the discharge conduit is continuously measured and after variation of the silver potential reaches 2.0 mV or less, the silver halide grains which are discharged from the discharge conduit, are introduced into the reaction vessel.

### Claim 11 (depends on 10)

The method of claim 10, wherein at least 50% of the total projected area of the silver halide grains which have been grown in the reaction vessel is accounted for by monodisperse tabular grains having an aspect ratio of not less than 5, an average grain diameter of not less than 0.6 .mu.m and a variation coefficient of grain size of not more than 20%.