Process for the partial reconstruction of the refractory lining of the wall of steel casting ladles
AssigneeDolomitwerke GmbH
InventorsHeinz Stripp, Wolfgang Rasim, Horst Tiemann
Life of this patent
Estimating the term…
Abstract
It was difficult until now to carry out intermediate repairs of monolithic refractory lining walls of steel casting and handling ladles when the slag area of the lining was worn before other areas. According to this new process for reconstructing the refractory lining in the upper area of the wall, repairs may be economically carried out in that the gap between the lower end of the template and the lining that projects under the area to be reconstructed is sealed by inflating a hose-like sealing body and by deflating again the sealing body before removing the template. This process is useful for steel casting and handling ladles and for similar metallurgical vessels.
Claims8
A method of repairing a refractory lining of a metallurgical vessel, the refractory lining having a bottom, a first wall region and a second wall region, the first wall region having an area to be repaired, the second wall region being disposed adjacent the bottom and the first wall region being disposed adjacent the second wall region;
- the method comprising the steps of:
- positioning a template adjacent the first wall region of the refractory lining of the metallurgical vessel;
- positioning a means for blocking castable refractory mix adjacent at least a portion of the second wall region of the metallurgical vessel;
- blocking the second wall region of the metallurgical vessel with the blocking means to minimize castable refractory mix leaving the area to be repaired of the first wall region;
- pouring castable refractory mix into the area to be repaired of the first wall region;
- and
- permitting the castable refractory mix to set in the area to be repaired of the first wall region.
A method of repairing a refractory lining of a metallurgical vessel, with an apparatus, the refractory lining having a bottom, a first wall region and a second wall region, the first wall region having an area to be repaired, the second wall region being disposed adjacent the bottom and the first wall region being disposed adjacent the second wall region;
- said apparatus comprising:
- a template for being disposed adjacent the first wall region of the metallurgical vessel to form an annular space for receiving castable refractory mix, the template having a ring-shaped cross-section;
- and means for blocking the second wall region and for minimizing leakage of castable refractory mix from the area to be repaired;
- the method comprising the steps of:
- providing the template;
- providing castable refractory mix;
- and
- providing the means for blocking the second wall region and for minimizing leakage of castable refractory mix from the area to be repaired;
- the method further comprising the steps of:
- positioning the template adjacent the first wall region of the refractory lining of the metallurgical vessel;
- positioning the means for blocking castable refractory mix adjacent at least a portion of the second wall region of the metallurgical vessel;
- blocking the second wall region of the metallurgical vessel with the blocking means to minimize castable refractory mix leaving the area to be repaired of the first wall region;
- pouring the castable refractory mix into the area to be repaired of the first wall region;
- and
- permitting the castable refractory mix to set in the area to be repaired of the first wall region.