# US 5,865,950 A · Process for creping tissue paper

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,865,950 A
- Document ID: US5865950A
- Status: Granted
- Kind: A
- Application number: 08/651,354
- Filed: 1996-05-22
- Granted: 1999-02-02
- Earliest claimed: 1996-05-22
- Assignees: The Procter & Gamble Company
- Inventors: Kenneth Douglas Vinson; Khosrow Parviz Mohammadi; Paul Thomas Weisman
- Web page: https://patentgrep.com/patent/US5865950A

## CPC

- C09J 103/08: Ethers
- B31F 1/12: Crêping
- C08G 73/0286: {Preparatory process from polyamidoamines and epihalohydrins}
- D21H 21/146: {Crêping adhesives}
- D21H 17/29: cationic
- D21H 17/36: Polyalkenyalcohols; Polyalkenylethers; Polyalkenylesters
- D21H 17/55: Polyamides; Polyaminoamides; Polyester-amides
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B31F: MECHANICAL WORKING OR DEFORMATION OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUS TO PAPER (making layered products not composed wholly of paper or cardboard B32B)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

A process for dry creping tissue paper comprising the application of creping adhesives in at least two steps. The adhesive applied in at least one of the steps is a polyvinyl alcohol while the adhesive applied in at least one other step comprises a water-soluble, thermosetting, cationic polyamide resin. The process provides high adhesion and doctorability for dry creping.

## Claims

### Claim 1

A process for creping a tissue paper web from a heated drying surface comprising the steps of:
a) providing a semi-dry embryonic tissue paper web wherein said semi-dry embryonic tissue paper web is comprised of a wet laid web that is dried to less than about 40% moisture content;
b) applying a first creping adhesive to the heated drying surface or to said semi-dry web, said first adhesive comprising a polyvinyl alcohol which forms an adhesive film and which has a degree of hydrolysis of at least about 80%;
c) applying a second creping adhesive to the heated drying surface or to said semi-dry web, said second adhesive comprising a water-soluble, thermosetting, cationic polyamide resin wherein said water-soluble, thermosetting, cationic polyamide resin is added in sufficient amount to comprise from about 5% to about 50% by weight based on the solid weight of said water-soluble, thermosetting, cationic polyamide resin relative to the solid weight of the total applied creping adhesive composition, adding said polyvinyl alcohol in an amount sufficient to comprise from about 30% to about 95% by weight based on the solid weight of said polyvinyl alcohol relative to the solid weight of the total applied creping adhesive composition and applying the total creping adhesive composition at a rate of about 0.1 to about 10 pounds per ton based on the dry weight of the total creping adhesive composition and the dry weight of said semi-dry web;
d) securing said semi-dry embryonic web by means of said first and second creping adhesives to the surface of said heated drying surface whereupon drying of said embryonic web is completed;
e) creping the dry web from said heated drying surface by means of a flexible creping blade.

### Claim 2 (depends on 1)

The process of claim 1 in which said polyvinyl alcohol is added in sufficient amount to comprise from about 75% to about 85% by weight based on the solid weight of the polyvinyl alcohol relative to the solid weight of the total applied creping adhesive.

### Claim 3 (depends on 1)

The process of claim 1 in which said water soluble, thermosetting, cationic polyamide resin is added in sufficient amount to comprise from about 15% to about 25% by weight based on the solid weight of polyamide resin relative to the solid weight of the total applied creping adhesive.

### Claim 4 (depends on 3)

The process of claim 3 in which said polyvinyl alcohol is added in sufficient amount to comprise from about 75% to about 85% by weight based on the solid weight of the polyvinyl alcohol relative to the solid weight of the total applied creping adhesive.

### Claim 5 (depends on 1)

The process of claim 1 in which said polyvinyl alcohol possesses a degree of hydrolysis between about 80% and about 95%.

### Claim 6 (depends on 5)

The process of claim 5 in which said polyvinyl alcohol possesses a viscosity greater than about 35 cP.

### Claim 7 (depends on 1)

The process of claim 1 in which said water soluble, thermosetting, cationic polyamide resin is the reaction product of an epihalohydrin and a polyamide containing secondary amine groups, said secondary amine groups derived from a polyalkylene polyamine and a saturated aliphatic dibasic carboxylic acid, said carboxylic acid containing from about 3 to about 10 carbon atoms.

### Claim 8 (depends on 7)

The process of claim 7 in which said epihalohydrin is epichlorohydrin used in a ratio between about 0.5 to 1 and about 1.8 to 1 relative to the secondary amine groups.

### Claim 9 (depends on 1)

The process of claim 1 in which said polyvinyl alcohol is applied by spraying through a spray boom, said polyvinyl alcohol being an aqueous dispersion having a concentration between about 0.05% and about 2% at the point of application.

### Claim 10 (depends on 9)

The process of claim 9 in which said water-soluble, thermosetting, cationic polyamide resin is applied by spraying through a spray boom, said polyamide resin being an aqueous dispersion having a concentration between about 0.025% and about 1% at the point of application.

### Claim 11 (depends on 1)

The process of claim 1 wherein said semi-dry web is prepared by pattern densification wherein the water removal to form the semi-dry web is effected while the embryonic web is supported on a drying fabric comprising an array of supports.

### Claim 12 (depends on 11)

The process of claim 11 wherein said water removal is accomplished at least partially by means of thermal transfer using air forced through the web while it is in contact with said fabric.

### Claim 13 (depends on 1)

The process of claim 1 in which said polyvinyl alcohol possesses a degree of hydrolysis between about 80% and about 95% and a viscosity greater than about 35 cP.

### Claim 14 (depends on 13)

The process of claim 13 in which said water soluble, thermosetting, cationic polyamide resin is the reaction product of an epihalohydrin and a polyamide containing secondary amine groups, said secondary amine groups derived from a polyalkylene polyamine and a saturated aliphatic dibasic carboxylic acid, said acid containing from about 3 to about 10 carbon atoms, and said epihalohydrin is epichlorohydrin used in a ratio between about 0.5 to 1 and about 1.8 to 1 relative to the secondary amine groups.

### Claim 15 (depends on 14)

The process of claim 14 wherein, in step b), said polyvinyl alcohol is applied by spraying an aqueous dispersion of said polyvinyl alcohol onto said heated drying surface and wherein, in step c), said water-soluble, thermosetting, cationic polyamide resin is applied by spraying an aqueous dispersion of said polyamide resin onto said heated drying surface subsequent to said polyvinyl alcohol application of step b) or onto said semi-dry tissue paper web.

### Claim 16 (depends on 15)

The process of claim 15 in which said polyvinyl alcohol and said water-soluble, thermosetting, cationic polyamide resins are applied by spraying through separate spray booms, said polyvinyl alcohol having a concentration in aqueous dispersion between about 0.05% and about 2% at the point of application and said polyamide resin having a concentration in aqueous dispersion between about 0.025% and about 1% at the point of application.

### Claim 17 (depends on 1)

The process of claim 1 wherein, in step b), said polyvinyl alcohol is applied by spraying an aqueous dispersion of said polyvinyl alcohol onto said heated drying surface and wherein, in step c), said water-soluble, thermosetting, cationic polyamide resin is applied by spraying an aqueous dispersion of said polyamide resin onto said heated drying surface subsequent to said polyvinyl alcohol application of step b) or onto said semi-dry tissue paper web.

### Claim 18 (depends on 17)

The process of claim 17 in which said polyvinyl alcohol and said water-soluble, thermosetting, cationic polyamide resins are applied by spraying through separate spray booms, said polyvinyl alcohol having a concentration in aqueous dispersion between about 0.05% and about 2% at the point of application and said polyamide resin having a concentration in aqueous dispersion between about 0.025% and about 1% at the point of application.

### Claim 19 (depends on 18)

The process of claim 18 in which said polyvinyl alcohol is added in sufficient amount to comprise from about 30% to about 95% by weight based on the dry weight of the polyvinyl alcohol relative to the dry weight of the total applied creping adhesive and said water soluble, thermosetting, cationic polyamide resin is added in sufficient amount to comprise from about 5% to about 50% by weight based on the dry weight of polyamide resin relative to the dry weight of the total applied creping adhesive.

### Claim 20 (depends on 19)

The process of claim 19 in which said polyvinyl alcohol possesses a degree of hydrolysis between about 80% and about 95% and a viscosity greater than about 35 cP.

### Claim 21 (depends on 20)

The process of claim 20 in which said water soluble, thermosetting, cationic polyamide resin is the reaction product of an epihalohydrin and a polyamide containing secondary amine groups, said secondary amine groups derived from a polyalkylene polyamine and a saturated aliphatic dibasic carboxylic acid, said acid containing from about 3 to about 10 carbon atoms, and said epihalohydrin is epichlorohydrin used in a ratio between about 0.5 to 1 and about 1.8 to 1 relative to the secondary amine groups.