Thermoplastic resin composition comprising cation-modified acrylamide or methacrylamide copolymer
AssigneeDai-Ichi Kogyo Seiyaku Co., Ltd.
InventorsTakayuki Tsubaki, Hideyuki Sumi, Hiroshi Hotta
Life of this patent
Estimating the term…
Abstract
The present invention provides a cation-modified linear copolymer which comprises, within the molecule thereof, 95 to 85 mole % of an ethylene structural unit, 0.1 to 10 mole % of an ester structural unit represented by general formula (II), 0.1 to 6 mole % of an acrylic or methacrylic acid structural unit and 1 to 12 mole % of an amide structural unit represented by general formula (IV). The copolymer and has a weight-average molecular weight of 1,000 to 100,000. When incorporated in thermoplastic resins, it shows good compatibility and results in good mechanical properties. ##STR1##
Claims3
A thermoplastic resin composition comprising a thermoplastic resin and a cation-modified linear copolymer which comprises, within the molecule thereof,
- 95 to 85 mole percent of an ethylene structural unit represented by the formula (I),
- 0.1 to 1 0 mole percent of an ester structural unit represented by the general formula (II),
- 0.1 to 6 mole percent of a carboxylic acid structural unit represented by the general formula (III) and 1 to 12 mole percent of an amide structural unit represented by the general formula (IV):
- ##STR7## wherein, in the above formulas, R.sup.1, R.sup.3 and R.sup.4 each independently represents a hydrogen atom or a methyl group, R.sup.2 represents an alkyl group containing 1 to 4 carbon atoms, R.sup.5 represents an alkylene group containing 2 to 8 carbon atoms, R.sup.6 and R.sup.7 each independently represents an alkyl group containing 1 to 4 carbon atoms, R.sup.8 represents an alkyl group containing 1 to 18 carbon atoms or an arylalkyl or aryl group containing 6 to 8 carbon atoms, and X.sup.- represents R.sup.9 SO.sub.3.sup.- in which R.sup.9 represents an alkyl group containing 1 to 12 carbon atoms or an arylalkyl or aryl group containing 6 to 18 carbon atoms, said copolymer having a weight-average molecular weight of 1,000 to 100,000.
A thermoplastic resin composition comprising a thermoplastic resin and a cation-modified linear copolymer which comprises, within the molecule thereof,
- 95 to 85 mole percent of an ethylene structural unit represented by the formula (I),
- 0.1 to 10 mole percent of an ester structural unit represented by the general formula (II) and 1 to 12 mole percent of an amide structural unit represented by the general formula (IV):
- ##STR8## wherein, in the above formulas, R.sup.1 and R.sup.4 each independently represents a hydrogen atom or a methyl group, R.sup.2 represents an alkyl group containing 1 to 4 carbon atoms, R.sup.5 represents an alkylene group containing 2 to 8 carbon atoms, R.sup.6 and R.sup.7 each independently represents an alkyl group containing 1 to 4 carbon atoms, R.sup.8 represents an alkyl group containing 1 to 18 carbon atoms or an arylalkyl or aryl group containing 6 to 8 carbon atoms, and X.sup.- represents R.sup.9 SO.sub.3.sup.- in which R.sup.9 represents an alkyl group containing 1 to 12 carbon atoms or an arylalkyl or aryl group containing 6 to 18 carbon atoms, said copolymer having a weight-average molecular weight of 1,000 to 100,000.