Polyester staple fibers of filaments with high resistance to pilling
AssigneeAkzo Nobel N.V.
InventorsJoseph C. W. Spijkers, Eberhard Ruf, Diederich Schilo
Life of this patent
Estimating the term…
Loading patent…
AssigneeAkzo Nobel N.V.
InventorsJoseph C. W. Spijkers, Eberhard Ruf, Diederich Schilo
Estimating the term…
Polyester staple fibers with high resistance to pilling contain (1) a polyester component consisting of at least 90 mol % polyethylene terephthalate, after its polycondensation, and (2) 1 to 7% by weight, relative to the polyester component, of a polyalkylene glycol block polymer with the formula ##STR1## in which the polyoxypropylene core has a mean molecular weight of 3000 to 4000 and a, b and c are integers such that the polyoxyethylene groups form 20 to 60% by weight of the block polymer, which has a mean molecular weight of 3750 to 10000. The staple fibers are prepared by admixing the polyester component and the block copolymer evenly in a separate phase and spinning the two together in the usual manner. The polyester component preferably is polyethylene terephthalate homopolyester, to which 2-4% by weight of the block copolymer is admixed.
Polyester staple fibers or filaments with high resistance to pilling, wherein the staple fibers or filaments comprise
Process for the manufacture of polyester staple fibers or filaments with high resistance to pilling, the process comprising evenly admixing in a separate phase
Dependencies are inferred from the claim text.