# US 5,858,491 A · Hollow molded articles and process for manufacturing them

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,858,491 A
- Document ID: US5858491A
- Status: Granted
- Kind: A
- Application number: 08/917,055
- Filed: 1997-08-22
- Granted: 1999-01-12
- Earliest claimed: 1994-11-02
- Assignees: Dow Belgium; Dow Europe GmbH
- Inventors: Theo L. V. Geussens; Herbert Bongartz; Jozef J. I. Van Dun
- Web page: https://patentgrep.com/patent/US5858491A

## CPC

- C08L 23/06: Polyethylene
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2314/02: Ziegler natta catalyst
- C08L 2314/06: Metallocene or single site catalysts
- Y10T 428/139: Open-ended, self-supporting conduit, cylinder, or tube-type article
- Y10T 428/1397: Single layer [continuous layer]
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Hollow molded articles prepared from a molding composition comprising: (A) from 95 to 60 percent by weight, based on the weight of (A) and (B), of an ethylene polymer having a density of 0.955 g/cm.sup.3 or higher, a melt index from 0.3 to 10 g/10 min, a melt index ratio I.sub.21 /I.sub.2 of from 40 to 80, and a polydispersity of from 1.8 to 10, the ethylene polymer being selected from the group consisting of i) high density ethylene homopolymers and ii) high density ethylene copolymers prepared by slurry or gas phase polymerization in the presence of a Ziegler or Phillips catalyst or prepared by polymerization in the presence of a transition metal compound catalyst containing a cyclopentadienyl or cyclopentadienyl derivative moiety; and (B) from 5 to 40 percent by weight, based on the weight of (A) and (B), of a homogeneous linear or substantially linear ethylene interpolymer having a density from 0.85 to 0.93 g/cm.sup.3, a melt index from 0.5 to 5 g/10 min, and a polydispersity of from 1.8 to 2.5 , the ethylene interpolymer being an interpolymer of at least ethylene and an .alpha.-olefin; wherein the composition has a density from 0.94 to 0.962 g/cm.sup.3 ; and a process of manufacturing hollow molded articles by molding such composition are claimed.

## Claims

### Claim 1

A hollow molded article prepared from a molding composition comprising:
(A) from 95 to 60 percent by weight, based on the weight of (A) and (B), of an ethylene polymer having a density of 0.955 g/cm.sup.3 or higher, a melt index from 0.3 to 10 g/10 min, a melt index ratio I.sub.21 /I.sub.2 of from 40 to 80, and a polydispersity of from 1.8 to 10, the ethylene polymer being selected from the group consisting of i) high density ethylene homopolymers and ii) high density ethylene copolymers prepared by slurry or gas phase polymerization in the presence of a Ziegler or Phillips catalyst or prepared by polymerization in the presence of a transition metal compound catalyst containing a cyclopentadienyl or cyclopentadienyl derivative moiety; and
(B) from 5 to 40 percent by weight, based on the weight of (A) and (B), of a homogeneous linear or substantially linear ethylene interpolymer having a density from 0.85 to 0.93 g/cm.sup.3, a melt index from 0.5 to 5 g/10 min, and a polydispersity of from 1.8 to 2.5 , the ethylene interpolymer being an interpolymer of at least ethylene and an .alpha.-olefin;
wherein the composition has a density from 0.94 to 0.962 g/cm.sup.3.

### Claim 2 (depends on 1)

The hollow molded article of claim 1 wherein (A) has a density of 0.960 g/cm.sup.3 or higher.

### Claim 3 (depends on 1)

The hollow molded article of claim 1 wherein (A) has a melt index from 0.5 to 3 g/10 min.

### Claim 4 (depends on 1)

The hollow molded article of claim 1 wherein (A) has a polydispersity of from 1.8 to 8.

### Claim 5 (depends on 1)

The hollow molded article of claim 1 wherein (B) has a density from 0.865 to 0.920 g/cm.sup.3.

### Claim 6 (depends on 1)

The hollow molded article of claim 1 wherein (B) has a density from 0.865 to 0.915 g/cm.sup.3.

### Claim 7 (depends on 1)

The hollow molded article of claim 1 wherein (B) has a melt index from 0.5 up to 3 g/10 min.

### Claim 8 (depends on 1)

The hollow molded article of claim 1 wherein (B) is a substantially linear ethylene interpolymer.

### Claim 9 (depends on 1)

The hollow molded article of claim 1 comprising from 95 to 80 percent by weight of (A) and from 5 to 20 percent by weight of (B), based on the weight of (A) and (B).

### Claim 10 (depends on 1)

The hollow molded article of claim 1 having a density from 0.95 to 0.96 g/cm.sup.3.

### Claim 11 (depends on 1)

The hollow molded article of claim 1 in the shape of a hollow profile, bottle or tube.

### Claim 12 (depends on 1)

The hollow molded article of claim 1 wherein (B) is a substantially linear ethylene interpolymer.

### Claim 13

A process of manufacturing hollow molded articles by molding a composition comprising
(A) from 95 to 60 percent by weight, based on the weight of (A) and (B), of an ethylene polymer having a density of 0.955 g/cm.sup.3 or higher, a melt index from 0.3 to 10 g/10 min, a melt index ratio I.sub.21 /I.sub.2 of from 40 to 80, and a polydispersity of from 1.8 to 10, the ethylene polymer being selected from the group consisting of i) high density ethylene homopolymers and ii) high density ethylene copolymers prepared by slurry or gas phase polymerization in the presence of a Ziegler or Phillips catalyst or prepared by polymerization in the presence of a transition metal compound catalyst containing a cyclopentadienyl or cyclopentadienyl derivative moiety; and
(B) from 5 to 40 percent by weight, based on the weight of (A) and (B), of a homogeneous linear or substantially linear ethylene interpolymer having a density from 0.85 to 0.93 g/cm.sup.3, a melt index from 0.5 to 5 g/10 min, and a polydispersity of from 1.8 to 2.5, the ethylene interpolymer being an interpolymer of at least ethylene and an .alpha.-olefin;
wherein the composition has a density from 0.94 to 0.962 g/cm.sup.3.

### Claim 14 (depends on 13)

The process of claim 13 wherein the composition is blow-molded.