# US 5,858,144 A · Low temperature joining of ceramic composites

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,858,144 A
- Document ID: US5858144A
- Status: Granted
- Kind: A
- Application number: 08/631,259
- Filed: 1996-04-12
- Granted: 1999-01-12
- Earliest claimed: 1996-04-12
- Assignees: Iowa State University Research Foundation, Inc.
- Inventors: Thomas J. Barton; Iver E. Anderson; Sina Ijadi-Maghsoodi; Mohammad Nosrati; Ozer Unal
- Web page: https://patentgrep.com/patent/US5858144A

## CPC

- C04B 41/5059: {Silicon carbide}
- C04B 37/005: {consisting of glass or ceramic material}
- C04B 37/006: {consisting of metals or metal salts}
- C04B 37/008: {by means of an interlayer consisting of an organic adhesive, e.g. phenol resin or pitch}
- C04B 41/009: {characterised by the material treated}
- C04B 41/87: Ceramics
- C04B 2235/5244: Silicon carbide
- C04B 2235/5256: Two-dimensional, e.g. woven structures
- C04B 2235/5268: Orientation of the fibers
- C04B 2235/528: Spheres
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/661: Multi-step sintering
- C04B 2235/665: Local sintering, e.g. laser sintering
- C04B 2237/083: Carbide interlayers, e.g. silicon carbide interlayers
- C04B 2237/121: based on aluminium
- C04B 2237/126: wherein the active component for bonding is not the largest fraction of the interlayer
- C04B 2237/128: The active component for bonding being silicon
- C04B 2237/36: Non-oxidic
- C04B 2237/365: Silicon carbide
- C04B 2237/366: Aluminium nitride
- C04B 2237/368: Silicon nitride
- C04B 2237/38: Fiber or whisker reinforced
- C04B 2237/708: of one or more of the interlayers
- C04B 2237/78: Side-way connecting, e.g. connecting two plates through their sides
- Y10S 977/776: Ceramic powder or flake
- Y10S 977/777: Metallic powder or flake
- Y10S 977/897: Polymerization
- Y10T 428/252: Glass or ceramic [i.e., fired or glazed clay, cement, etc.] [porcelain, quartz, etc.]
- Y10T 428/31678: Of metal
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of joining similar or dissimilar ceramic and ceramic composite materials, such as SiC continuous fiber ceramic composites, at relatively low joining temperatures uses a solventless, three component bonding agent effective to promote mechanical bond toughness and elevated temperature strength to operating temperatures of approximately 1200 degrees C. The bonding agent comprises a preceramic precursor, an aluminum bearing powder, such as aluminum alloy powder, and mixtures of aluminum metal or alloy powders with another powder, and and boron powder in selected proportions. The bonding agent is disposed as an interlayer between similar or dissimilar ceramic or cermaic composite materials to be joined and is heated in ambient air or inert atmosphere to a temperature not exceeding about 1200 degrees C. to form a strong and tough bond joint between the materials. The bond joint produced is characterized by a composite joint microstructure having relatively soft, compliant aluminum bearing particulate regions dispersed in a ceramic matrix.

## Claims

### Claim 1

A method of joining ceramic or ceramic composite materials, comprising disposing a bonding agent at an interface between said materials wherein the bonding agent comprises a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a joint comprising metallic phase regions comprising aluminum disposed in a ceramic joint material and heating the interface to a temperature not exceeding about 1200 degrees C. to form said joint between the materials.

### Claim 2 (depends on 1)

The method of claim 1 wherein the interface is heated in an air atmosphere.

### Claim 3 (depends on 2)

The method of claim 2 wherein the interface is heated by an open flame of a torch in the ambient air atmosphere.

### Claim 4 (depends on 1)

The method of claim 1 wherein the interface is heated in an inert atmosphere.

### Claim 5 (depends on 1)

The method of claim 1 wherein the aluminum bearing particulates are selected from elemental aluminum powder, aluminum alloy powder, and mixtures of elemental aluminum powder with a second powder.

### Claim 6 (depends on 1)

The method of claim 1 wherein the boron particulates comprise boron powder having a powder particle size below 1 micron.

### Claim 7 (depends on 1)

The method of claim 1 wherein the bonding agent comprises, in weight %, about 25% to 85% preceramic polymer, about 10% to 70% aluminum bearing powder, and about 2% to 6% boron powder.

### Claim 8 (depends on 1)

The method of claim 1 including forming second ceramic phase regions in a ceramic matrix of the ceramic joint material.

### Claim 9 (depends on 1)

The method of claim 1 wherein the ceramic composite material comprises SiC fibers disposed in a SiC matrix.

### Claim 10

A method of repairing ceramic or ceramic composite material, comprising filling a crack, hole or depression in the material with a bonding agent comprising a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a filler comprising metallic phase regions comprising aluminum disposed in a ceramic filler material and heating the bonding agent to a temperature not exceeding about 1200 degrees C. to form said filler in said crack, hole or depression.

### Claim 11 (depends on 10)

The method of claim 10 wherein the ceramic material comprises monolithic SiC.

### Claim 12 (depends on 10)

The method of claim 10 wherein the ceramic composite material comprises SiC fibers disposed in a SiC matrix.

### Claim 13 (depends on 10)

The method of claim 10 wherein the bonding agent comprises, in weight %, about 25% to 85% preceramic polymer, about 10% to 70% aluminum bearing powder, and about 2% to 6% boron powder.

### Claim 14 (depends on 10)

The method of claim 10 wherein the bonding agent is heated in an air atmosphere.

### Claim 15

A method of joining ceramic or ceramic composite materials, comprising disposing a bonding agent at an interface between said materials wherein the bonding agent comprises a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a joint comprising metallic phase regions comprising aluminum disposed in a ceramic joint material and heating the interface in an oxygen bearing atmosphere to a temperature not exceeding about 1200 degrees C. to form said joint between the materials.

### Claim 16

A method of repairing ceramic or ceramic composite material, comprising filling a crack, hole or depression in the material with a bonding agent comprising a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a filler comprising metallic phase regions comprising aluminum disposed in a ceramic filler material and heating the bonding agent in an oxygen bearing atmosphere to a temperature not exceeding about 1200 degrees C. to form said filler in the crack, hole or depression.