Macromonomers having reactive end groups
AssigneeMaxdem Incorporated
InventorsRobert R. Gagne, Matthew Louis Marrocco, III, Mark Steven Trimmer, Neil H. Hendricks
Life of this patent
Estimating the term…
Loading patent…
AssigneeMaxdem Incorporated
InventorsRobert R. Gagne, Matthew Louis Marrocco, III, Mark Steven Trimmer, Neil H. Hendricks
Estimating the term…
A soluble rigid-rod macromonomer is provided which has the following formula: ##STR1## wherein each A.sub.1, A.sub.2, A.sub.3, and A.sub.4, on each monomer unit, independently, is C or N, and each G.sub.1, G.sub.2, G.sub.3, and G.sub.4, on each monomer unit, independently, is H or a solubilizing side group, provided that at least one monomer unit has at least one solubilizing side group. The solubilizing side groups provide the macromonomers with a solubility of at least 0.5% by weight in the solvent system from which they are formed. E is a reactive end group, and the macromonomer has an average degree of polymerization, DP.sub.n, greater than 6. Such macromonomers are chemically incorporated into polymer systems to provide stronger stiffened polymers.
A rigid-rod macromonomer of the formula:
A rigid-rod macromonomer of the formula:
A rigid-rod macromonomer of the formula:
A rigid-rod macromonomer of the formula:
A soluble rigid-rod macromonomer of the formula:
Dependencies are inferred from the claim text.