Abstract
Sizing emulsions comprised of (a) hydrophobic cellulose-reactive sizing agents and (b) amines, amine salts and/or quaternary amines are disclosed, as well as low shear and high shear processes for making said emulsions and methods of using said emulsions for sizing paper.
Claims25
A composition comprised of
- (a) alkenyl succinic anhydride, and
- (b) about 3% to about 20%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of trialkyl amine of the formula (I), dimethyl sulfate quaternary salt of trialkyl amine of the formula (I), benzyl chloride quaternary salt of trialkyl amine of the formula (I), and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR4## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 14 to 24 carbon atoms, and
- wherein said composition contains about 0.1% water or less.
A composition consisting essentially of
- (a) alkenyl succinic anhydride, and
- (b) about 3% to about 20%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of trialkyl amine of the formula (I), dimethyl sulfate quaternary salt of trialkyl amine of the formula (I), benzyl chloride quaternary salt of trialkyl amine of the formula (I), and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR5## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 14 to 24 carbon atoms.
A composition comprised of
- (a) alkenyl succinic anhydride,
- (b) about 3% to about 20%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of trialkyl amine of the formula (I), dimethyl sulfate quaternary salt of trialkyl amine of the formula (I), benzyl chloride quaternary salt of trialkyl amine of the formula (I), and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR6## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 14 to 24 carbon atoms,
- (c) water, and
- (d) an inorganic salt,
- wherein said alkenyl succinic anhydride is dispersed in said water to form an emulsion,
- wherein said inorganic salt is present in an amount effective to reduce the droplet size of said emulsion, and
- wherein said emulsion has a pH value effective to provide an emulsion average droplet size of about 3 microns or less.
4 more elements
A composition comprised of
- (a) alkenyl succinic anhydride,
- (b) about 4% to about 10%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of dimethyl sulfate quaternary salt of trialkyl amine of the formula (I) and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR7## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 16 to 18 carbon atoms,
- (c) water, and
- (d) a sulfate salt,
- wherein said alkenyl succinic anhydride is dispersed in said water to form an emulsion,
- wherein said sulfate salt is present in an amount effective to reduce the droplet size of said emulsion, and
- wherein said emulsion has a pH value of about 4.0 or lower.
4 more elements
A process comprising mixing
- (a) alkenyl succinic anhydride,
- (b) about 3% to about 20%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of trialkyl amine of the formula (I), dimethyl sulfate quaternary salt of trialkyl amine of the formula (I), benzyl chloride quaternary salt of trialkyl amine of the formula (I), and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR8## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 14 to 24 carbon atoms,
- (c) water, and
- (d) an inorganic salt, to form an emulsion,
- wherein said inorganic salt is present in an amount effective to reduce the droplet size of said emulsion, and
- wherein said emulsion has a pH value effective to provide an emulsion average droplet size of about 3 microns or less.
3 more elements
A process comprising mixing
- (a) a composition comprised of
- (i) alkenyl succinic anhydride, and
- (ii) about 3% to about 20%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of trialkyl amine of the formula (I), dimethyl sulfate quaternary salt of trialkyl amine of the formula (I), benzyl chloride quaternary salt of trialkyl amine of the formula (I), and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR9## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 14 to 24 carbon atoms;
- (b) water;
- and
- (c) an inorganic salt to form an emulsion,
- wherein said inorganic salt is present in an amount effective to reduce the droplet size of said emulsion, and
- wherein said emulsion has a pH value effective to provide an emulsion average droplet size of about 3 microns or less.
5 more elements
A process comprising mixing
- (a) alkenyl succinic anhydride,
- (b) about 4% to about 10%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of dimethyl sulfate quaternary salt of trialkyl amine of the formula (I) and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR10## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 16 to 18 carbon atoms,
- (c) water, and
- (d) a sulfate salt, to form an emulsion,
- wherein said sulfate salt is present in an amount effective to reduce the droplet size of said emulsion,
- wherein said emulsion has a pH value of about 4.5 or lower, and
- wherein said mixing is carried out at low shear.
4 more elements
A method comprising
- (a) providing paper stock;
- (b) providing a composition comprised of
- (i) alkenyl succinic anhydride,
- (ii) about 3% to about 20%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of trialkyl amine of the formula (I), dimethyl sulfate quaternary salt of trialkyl amine of the formula (I), benzyl chloride quaternary salt of trialkyl amine of the formula (I), and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR11## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 14 to 24 carbon atoms,
- (iii) water, and
- (iv) an inorganic salt,
- wherein said alkenyl succinic anhydride is dispersed in said water to form an emulsion,
- wherein said inorganic salt is present in an amount effective to reduce the droplet size of said emulsion, and
- wherein said emulsion has a pH value effective to provide an emulsion average droplet size of about 3 microns or less;
- (c) forming a web from said paper stock;
- and
- (d) mixing said emulsion with said paper stock or applying said emulsion to said web, in an amount effective to size paper that is formed from said web.
9 more elements
A method comprising
- (a) providing paper stock;
- (b) providing a composition comprised of
- (i) alkenyl succinic anhydride,
- (ii) about 4% to about 10%, by weight based on said alkenyl succinic anhydride, of an amine selected from the group consisting of trialkyl amine of the formula (I), dimethyl sulfate quaternary salt of trialkyl amine of the formula (I), benzyl chloride quaternary salt of trialkyl amine of the formula (I), and diethyl sulfate quaternary salt of trialkyl amine of the formula (I), ##STR12## wherein R.sub.1 is methyl or ethyl, R.sub.2 is methyl or ethyl, and R.sub.3 is alkyl having 16 to 18 carbon atoms,
- (iii) water, and
- (iv) an inorganic salt,
- wherein said alkenyl succinic anhydride is dispersed in said water to form an emulsion,
- wherein said composition is formed by mixing said (i), (ii), (iii), and (iv) at low shear,
- wherein said inorganic salt is present in an amount effective to reduce the droplet size of said emulsion, and
- wherein said emulsion has a pH value of about 4.5 or lower;
- (c) forming a web from said paper stock;
- and
- (d) applying said emulsion to said web, in an amount effective to size paper that is formed from said web, by a method selected from the group consisting of spraying and size pressing.
10 more elements