Low- and high-molecular weight amorphous polyalphaolefin polymer blends having high melt viscosity, and products thereof
AssigneeRexene Corporation
InventorAndres Sustic
Life of this patent
Estimating the term…
Loading patent…
AssigneeRexene Corporation
InventorAndres Sustic
Estimating the term…
A polymer blend having an open time including a high molecular weight average, predominantly atactic flexible polyolefin polymer having a heat of fusion of about 15 to 60 J/g, and a low molecular weight average, atactic polyolefin polymer having a heat of fusion of about 0.1 to 20 J/g, wherein the high molecular weight polymer and low molecular weight polymer are sufficiently miscible to impart a single glass transition temperature to the polymer blend, and the low molecular weight polymer is present in an amount sufficient to impart a melt viscosity of greater than about 8,000 cPs at room temperature and a crystallinity below about 25 J/g to the polymer blend. The invention further includes methods for preparing such polymer blends, and the products produced from the polymer blends, which are useful for hot melt adhesives, asphalt and bitumen applications such as roofing membranes, polymeric modifiers and the like.
A polymer blend comprising:
A method of preparing a polymer blend comprising combining a high weight average molecular weight, predominantly atactic flexible polyolefin polymer having a heat of fusion of about 15 to 60 J/g and a low number average molecular weight, atactic polyolefin polymer having a heat of fusion of about 0.1 to 20 J/g by heating the high molecular weight polymer and low molecular weight polymer until they are sufficiently miscible to impart a single glass transition temperature and an open time to the polymer blend, wherein the low molecular weight polymer is present in an amount sufficient to impart a melt viscosity of greater than about 8,000 cPs at room temperature and a crystallinity below about 28 J/g to the polymer blend.
Dependencies are inferred from the claim text.