Abstract
The present invention relates to a process for the production of molded articles via the reaction injection molding technique. According to the RIM process, a reaction mixture is introduced into a closed mold, allowed to react fully, and removed from the mold. More specifically, these reaction mixtures comprise an isocyanate-reactive material, a chain extender, and a stable, liquid diallophanate modified diphenylmethane diisocyanate (MDI). Two specific processes for the preparation of the suitable diallophanate modified diisocyanate are disclosed. These diallophanate modified isocyanates either have an isocyanate group content from about 12 to 30%, or from about 5 to 29%.
Claims13
A process for producing a molded article via the reaction injection molding (RIM) technique by introducing a reaction mixture into a closed mold, wherein said reaction mixture has an isocyanate index of from about 80 to 120 and said reaction mixture comprises:
- A) an isocyanate-reactive material,
- B) a chain extender, and
- C) a stable, liquid diallophanate-modified diphenylmethane diisocyanate prepared by either:
- 1) (a) reacting
- (i) one equivalent of a diisocyanate, with
- (ii) one equivalent of an aliphatic alcohol containing 1 to 36 carbon atoms or aromatic alcohol containing 6 to 18 carbon atoms wherein the hydroxyl group is directly attached to the aromatic ring to form a diurethane of the diisocyanate,
- (b) reacting said diurethane with a diphenylmethane diisocyanate isomer composition comprising about 0 to 60% by weight of 2,4'-diphenylmethane diisocyanate and less than 6% by weight of 2,2'-diphenylmethane diisocyanate with the remainder being 4,4'-diphenylmethane diisocyanate, in the presence of an allophanate catalyst to yield said stable, liquid diallophanate-modified diphenylmethane diisocyanate, followed by the addition of a catalyst stopper,
- wherein said stable, liquid diallophanate-modified diphenylmethane diisocyanate has an isocyanate group content of from 12.0 to 30.0%;
- or
- (a) reacting
- (i) one equivalent of a diisocyanate, with
- (ii) one equivalent of an aliphatic alcohol containing 1 to 36 carbon atoms or aromatic alcohol containing 6 to 18 carbon atoms to form a diurethane of the diisocyanate,
- (b) reacting said diurethane with a diphenylmethane diisocyanate isomer composition comprises about 0 to 60% by weight of 2,4'-diphenylmethane diisocyanate and less than 6% by weight of 2,2'-diphenylmethane diisocyanate with the remainder being 4,4'-diphenylmethane diisocyanate, in the presence of an allophanate catalyst to yield a diallophanate-modified diphenylmethane diisocyanate having an isocyanate group content of from 12.0 to 30%, followed by the addition of a catalyst stopper, and
- (c) reacting said diallophanate-modified diphenylmethane diisocyanate having an isocyanate group content of from 12.0 to 30.0%, with at least one compound selected from the group consisting of:
- (i) an organic material containing about 1.8 or more hydroxy, primary amine or secondary amine groups or any combination thereof, having a molecular weight of from 400 to 6000, (ii) a diol having a molecular weight of from 60 to 200 and (iii) mixtures of (i) and (ii), to form said stable, liquid diallophanate modified isocyanate wherein said diallophanate-modified isocyanate has an isocyanate group content of from 5 to 29%;
- allowing said reaction mixture to fully react, and removing the molded article from the mold.
Dependencies are inferred from the claim text.