# US 5,585,314 A · Method of making in-situ grown whisker reinforced ceramics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,585,314 A
- Document ID: US5585314A
- Status: Granted
- Kind: A
- Application number: 08/423,756
- Filed: 1995-04-18
- Granted: 1996-12-17
- Earliest claimed: 1994-06-23
- Assignees: Cercom, Inc.
- Inventors: Andre Ezis; C. James Shih
- Web page: https://patentgrep.com/patent/US5585314A

## CPC

- C04B 35/593: obtained by pressure sintering
- C04B 35/575: obtained by pressure sintering
- C04B 35/80: Fibres, filaments, whiskers, platelets, or the like
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

In-situ Si.sub.3 N.sub.4 whisker growth mechanisms have enhanced the microstructure of ceramic materials such as SiC through controlled growth of elongated beta-type Silicon Nitride grains. During liquid phase sintering at temperatures not exceeding 1850.degree. C., alpha-type Silicon Nitride dissolves into the liquid phase and reprecipitates as an elongated or acicular beta modification. The Si.sub.3 N.sub.4 reinforced microstructures can be formed by the controlled recrystallization of beta-type Silicon Nitride. In-situ whisker growth is enhanced or optimized through the use of thermal treatments and/or additions of seed materials. Finely divided beta-type Silicon Nitride particles which are insoluble in the liquid phase during sintering, and therefore have been used to provide nucleation sites for whisker growth are employed. Thermal treatments have been designed to promote directional growth (elongation) as opposed to development of less elongated type grains.

## Claims

### Claim 1

A method of making a ceramic material, comprising:
a) providing a ceramic powder mixture consisting essentially of SiC powder and 1% to 50%, by weight, Si.sub.3 N.sub.4 powder;
b) providing a sintering aid comprising a powdered composition facilitating liquid phase sintering at or below 1850.degree. C.;
c) blending said ceramic powder mixture and sintering aid into a homogeneous mixture;
d) liquid phase sintering said homogeneous mixture at a temperature above a melting temperature of said sintering aid but at a temperature no greater than 1850.degree. C. for a time period sufficient to facilitate said Si.sub.3 N.sub.4 powder going into solution within said homogeneous mixture;
e) recrystallizing Si.sub.3 N.sub.4 material as acicular whiskers uniformly dispersed within said ceramic material.

### Claim 2 (depends on 1)

The method of claim 1, wherein said step of providing a ceramic powder mixture comprises the step of providing alpha Si.sub.3 N.sub.4 powder.

### Claim 3 (depends on 2)

The method of claim 2, wherein said ceramic powder consists essentially of either alpha or beta SiC powder, said Si.sub.3 N.sub.4 powder comprising predominantly alpha Si.sub.3 N.sub.4 powder with up to 5% addition, by weight, beta Si.sub.3 N.sub.4 powder.

### Claim 4 (depends on 1)

The method of claim 1, wherein said sintering aid comprise a mixture of Y.sub.2 O.sub.3 and Al.sub.2 O.sub.3.

### Claim 5 (depends on 4)

The method of claim 4, wherein said sintering aid also includes SiO.sub.2.

### Claim 6 (depends on 4)

The method of claim 4, wherein said sintering aid includes 60%, by weight, Al.sub.2 O.sub.3 and 40%, by weight, Y.sub.2 O.sub.3.

### Claim 7 (depends on 1)

The method of claim 1, wherein said ceramic powder mixture has an average particle size less than 1 micrometer.

### Claim 8 (depends on 7)

The method of claim 7, wherein said ceramic powder mixture has a surface area to weight ratio of about 15 m.sup.2 /g.

### Claim 9 (depends on 1)

The method of claim 1, wherein said liquid phase sintering is conducted at a pressure less than 3500 psi.

### Claim 10 (depends on 1)

The method of claim 1, wherein after said recrystallizing, said method includes the step of heat treating in a Nitrogen atmosphere.

### Claim 11 (depends on 10)

The method of claim 10, wherein said step of heat treating is conducted at a temperature about 1800.degree. C.