# US 5,573,057 A · Camshaft and method for casting the camshaft

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,573,057 A
- Document ID: US5573057A
- Status: Granted
- Kind: A
- Application number: 08/204,365
- Filed: 1994-03-15
- Granted: 1996-11-12
- Earliest claimed: 1991-09-19
- Assignees: Lydmet Limited
- Inventors: Alexander K. McDonald
- Web page: https://patentgrep.com/patent/US5573057A

## CPC

- C21D 5/00: Heat treatments of cast-iron
- B22D 15/00: Casting using a mould or core of which a part significant to the process is of high thermal conductivity, e.g. chill casting; Moulds or accessories specially adapted therefor
- F16H 53/02: Single-track cams for single-revolution cycles; Camshafts with such cams
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- F16H: GEARING

## Abstract

A method of producing a chilled iron camshaft from a chromium containing cast iron is described. The cast iron material contains between 0.5 wt % to 1.2 wt % of chromium. The camshaft having a white iron structure adjacent chill inserts in a casting mold and a grey iron structure in substantially all other regions remote from the chills. The method comprising the steps of assembling a sand casting mold having a camshaft shaped cavity and also having chill inserts adjacent the cavity regions where white iron is desired. Preparing a molten metal charge of cast iron having a carbon equivalent lying in the range from 3.5 up to 4.0 wt % and adding sufficient nucleant prior to pouring to fill the mold cavity, to ensure that under cooling of residual liquid remaining after solidification of the white iron structure adjacent the chills remains above the iron-cementite eutectic temperature prior to solidification into grey iron.

## Claims

### Claim 1

A method of producing a cast-iron camshaft from an iron material containing between 0.3 wt % and 1.2 wt % of chromium by a chill cashing technique, the camshaft having a region of white iron structure formed adjacent chill inserts in a casting mold and a region of grey iron structure in substantially all other regions remote from the chill inserts said all other regions comprising a central core, the method comprising the steps of (1) assembling a casting mold having a camshaft shaped cavity and also having chill inserts adjacent cavity regions where white iron is desired, said chill inserts forming a contact surface for cast molten metal around at least part of an outer periphery of a cam portion of said camshaft, (2) preparing a molten metal charge of cast iron having a carbon equivalent lying in the range from 3.5 up to 4.0, (3) adding an amount of nucleant material to said molten metal charge prior to a metal pouring step, said amount of nucleant material being in excess of that theoretically required to cause still molten metal remote from said chill inserts lying within the white iron region to solidify as grey iron; and (4) casting said molten charge of cast iron into said casting mold, said excess amount of nucleant material serving to ensure that undercooling of residual liquid remaining in said central core of said camshaft after solidification of the white iron region around said residual liquid and adjacent the chill inserts remains above an iron-cemenite eutectic temperature so that it solidifies as said region of grey iron structure wherein carbon is present as free graphite, whereby to ensure that said central core of said camshaft is substantially froe of white iron structure.

### Claim 2 (depends on 1)

A method according to claim 1 characterised in that the carbon equivalent comprises from 3.0 wt % to 3.6 wt % of carbon.

### Claim 3 (depends on 2)

A method according to claim 2 characterised in that the chromium content of the iron lies in the range from 0.5 wt % to 0.9 wt %.

### Claim 4 (depends on 3)

A method according to claim 3 characterised in that the iron contains up to 1.5 wt % of copper.

### Claim 5 (depends on 4)

A method according to claim 4 characterized in that the cast iron composition lies in the range in wt %, carbon: 3.3-3.4, silicon: 1.5-1.6, chromium: 0.7-0.8, molybdenum: 0-0.25, nickel: 0-0.25, copper: 0.6-0.8, iron: balance.

### Claim 6 (depends on 4)

A method according to claim 4 characterized in that the cast iron composition lies in the range, in wt %, carbon: 3.15-3.35, silicon: 1.7-1.8, chromium: 0.8-0.9, molybdonum: 0-0.25. nickel: 0-0.25, copper: 0.6-0.8, iron balance.