# US 5,569,723 A · Process for the bromination of alkyl rubbers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,569,723 A
- Document ID: US5569723A
- Status: Granted
- Kind: A
- Application number: 08/543,138
- Filed: 1995-10-13
- Granted: 1996-10-29
- Earliest claimed: 1994-10-24
- Assignees: Bayer Aktiengesellschaft
- Inventors: Wolfgang Baade; Heinrich K onigshofen; Gabor Kaszas
- Web page: https://patentgrep.com/patent/US5569723A

## CPC

- C08C 19/14: by reaction with halogens
- B60C 1/0008: {Compositions of the inner liner}
- C08F 8/22: by reaction with free halogens
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

C.sub.4 -C.sub.16 alkyl rubbers are brominated by reacting the alkyl rubbers with bromine in the presence of organic azo compounds and/or alkali metal and/or alkaline earth metal hypochlorites and in the presence of linear, branched and/or cyclic alkanes and water at temperatures of 10.degree. to 100.degree. C., optionally under pressure, wherein the quantity of bromine is 0.2 to 1.2 times the molar quantity of double bonds contained in the rubber, 0.1 to 3 times the molar quantity of hypochlorite and/or azo compounds is used relative to the quantity of bromine used, providing that the concentration of the hypochlorites in an aqueous solution is 2 to 20 wt. %, and wherein 5 to 20 wt. % of water, 60 to 90 wt. % of alkanes and 5 to 25 wt. % of alkyl rubber are used relative to 100 wt. % of the total of alkyl rubber, alkanes and water.

## Claims

### Claim 1

Process for the bromination of C.sub.4 -C.sub.16 alkyl rubbers, characterised in that the alkyl rubbers are reacted with bromine in the presence of organic azo compounds and/or alkali metal and/or alkaline earth metal hypochlorites and in the presence of linear, branched and/or cyclic alkanes and water at temperatures of 10.degree. to 100.degree. C., optionally under pressure, wherein the quantity of bromine is 0.2 to 1.2 times the molar quantity of double bonds contained in the rubber, 0.1 to 3 times the molar quantity of hypochlorite and/or azo compound is used relative to the quantity of bromine used, providing that the concentration of the hypochlorites in an aqueous solution is 2 to 20 wt. %, and wherein 5 to 20 wt. % of water, 60 to 90 wt. % of alkanes and 5 to 25 wt. % of alkyl rubber are used relative to 100 wt. % of the total of alkyl rubber, alkanes and water.

### Claim 2 (depends on 1)

Process according to claim 1, characterised in that it is performed in the presence of sodium hypochlorite, potassium hypochlorite and/or magnesium hypochlorite.

### Claim 3 (depends on 1)

Process according to claim 1, characterised in that it is performed in the presence of azodiisobutyronitrile.

### Claim 4 (depends on 1)

Process according to claim 1, characterised in that it is performed in the presence of pentanes, hexanes, cyclohexanes and/or heptanes.

### Claim 5 (depends on 1)

Process according to claim 1, characterised in that it is performed at pressures of 0.8 to 10 bar.