# US 5,545,337 A · Ceramic coating system or water oxidation environments

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,545,337 A
- Document ID: US5545337A
- Status: Granted
- Kind: A
- Application number: 08/346,144
- Filed: 1994-11-29
- Granted: 1996-08-13
- Earliest claimed: 1994-11-29
- Assignees: Modar, Inc.
- Inventors: Glenn T. Hong
- Web page: https://patentgrep.com/patent/US5545337A

## CPC

- C02F 1/025: {Thermal hydrolysis}
- C02F 11/08: Wet air oxidation
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

A process for water oxidation of combustible materials in which during at least a part of the oxidation corrosive material is present and makes contact with at least a portion of the apparatus over a contact area on the apparatus. At least a portion of the contact surface area comprises titanium dioxide coated onto a titanium metal substrate. Such ceramic composites have been found to be highly resistant to environments encountered in the process of supercritical water oxidation. Such environments typically contain greater than 50 mole percent water, together with oxygen, carbon dioxide, and a wide range of acids, bases, and salts. Pressures are typically about 27.5 to about 1000 bar while temperatures range as high as 700.degree. C. The ceramic composites are also resistant to degradation mechanisms caused by thermal stresses.

## Claims

### Claim 1

A process for high temperature water oxidation of combustible material in a high temperature water oxidation apparatus, in which during at least part of the oxidation, corrosive material is present and contacts the apparatus over a contact area on the apparatus, the process comprising contacting in an aqueous phase the combustible material and an oxidizing agent under conditions suitable to cause oxidation of the combustible material, wherein the oxidation is at a temperature in the range of about 300.degree. C. to about 700.degree. C. and at pressures from about 27.5 bar (400 psi) to about 1000 bar (15,000 psi) and the contact area contains a ceramic composite comprising titanium base metal overlaid with a titania coating, to provide corrosion resistance from said corrosive material in said contact area.

### Claim 2 (depends on 1)

The process of claim 1 wherein the corrosive material comprises at least one moiety selected from the group consisting of Cl and SO.sub.4 and at least one moiety selected from the group consisting of H and Na.

### Claim 3 (depends on 2)

The process of claim 2 wherein the corrosive material comprises (i) at least one selected from the group consisting of HCl, H.sub.2 SO.sub.4, NaOH, Na.sub.2 CO.sub.3 and (ii) a sodium salt.

### Claim 4 (depends on 1)

The process of claim 1 wherein the aqueous phase containing the corrosive material and oxidizing agent contains greater than 50 mole percent water.

### Claim 5 (depends on 4)

The process of claim 4 wherein the aqueous phase further contains oxygen, carbon dioxide, acids, bases and salts.

### Claim 6 (depends on 1)

The process of claim 1 wherein the oxidation apparatus is a reactor selected from the group consisting of vessel reactors, hydraulic column reactors, and pipe reactors.

### Claim 7 (depends on 1)

The process of claim 1 wherein the titanium base metal is an alloy.

### Claim 8 (depends on 1)

The process of claim 1 wherein the titania coating of the ceramic composite consists of multiple layers, each successive layer from the titanium metal substrate having a smaller thermal coefficient.

### Claim 9 (depends on 1)

The process of claim 1 wherein the contact area further comprises a metallic bond coat between the titanium base metal and the overlying titania.

### Claim 10 (depends on 9)

The process of claim 9 wherein the metallic bond coat contains titanium.

### Claim 11 (depends on 9)

The process of claim 9 wherein the ceramic composite further comprises a cermet consisting of titanium dioxide and titanium between the metallic bond coat and the overlying titania.

### Claim 12 (depends on 11)

The process of claim 11 wherein the titanium of the cermet is an alloy.

### Claim 13 (depends on 1)

The process of claim 1 wherein the coating of the ceramic composite is applied onto the titanium base metal by thermal spraying of the titania.

### Claim 14

A process of oxidizing combustible materials containing corrosive constituents in an oxidation apparatus in which an aqueous phase containing the oxidizable combustible material and oxidizing agent is contacted with at least a portion of a contact area of the apparatus under conditions suitable to cause oxidation of the combustible material, at a temperature of at least about 300.degree. C. and a pressure of at least about 27.5 bar, wherein said corrosive constituents are present in said contact area, and wherein the contact area contains a ceramic composite consisting of titanium dioxide coated onto a titanium metal substrate to provide corrosion resistance from said corrosive constituents in said contact area.

### Claim 15 (depends on 14)

The process of claim 14 wherein the oxidation is conducted at a temperature in the range of about 300.degree. C. to about 700.degree. C.

### Claim 16 (depends on 15)

The process of claim 15 wherein the oxidation is conducted at a pressure within the range of from about 27.5 bar (400 psi) to about 1,000 bar (15,000 psi).

### Claim 17 (depends on 14)

The process of claim 14 wherein the titanium dioxide coating of the ceramic composite consists of multiple layers, each successive layer from the titanium metal substrate having a smaller thermal coefficient.

### Claim 18 (depends on 14)

The process of claim 14 wherein the contact area further comprises a metallic bond coat between the titanium base metal and the overlying cermet, wherein the cermet consists of titanium dioxide and titanium and further wherein the cermet is between the metallic bond coat and the overlying titania.

### Claim 19

A process for oxidizing combustible material in a water oxidation apparatus, in which during at least part of the oxidation, corrosive material is present and contacts the apparatus over a contact area on the apparatus, the process comprising contacting in an aqueous phase the combustible material and an oxidizing agent under conditions suitable to cause oxidation of the combustible material at a temperature of at least about 300.degree. C. and a pressure of at least about 27.5 bar, wherein the contact area contains a ceramic composite comprising titanium base metal overlaid with a titania coating, to provide corrosion resistance from said corrosive material in said contact area.

### Claim 20 (depends on 19)

The process of claim 19 wherein the titania coating of the ceramic composite consists of multiple layers, each successive layer from the titanium metal substrate having a smaller thermal coefficient.