# US 5,527,471 A · Iridium material for hydrothermal oxidation environments

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,527,471 A
- Document ID: US5527471A
- Status: Granted
- Kind: A
- Application number: 08/382,674
- Filed: 1995-02-02
- Granted: 1996-06-18
- Earliest claimed: 1995-02-02
- Assignees: Modar, Inc.
- Inventors: Glenn T. Hong; Vladimir A. Zilberstein
- Web page: https://patentgrep.com/patent/US5527471A

## CPC

- G21C 3/07: characterised by their material, e.g. alloys
- B01J 3/008: {Processes carried out under supercritical conditions}
- B01J 3/04: Pressure vessels, e.g. autoclaves
- B01J 19/02: Apparatus characterised by being constructed of material selected for its chemically-resistant properties
- C02F 11/08: Wet air oxidation
- C02F 11/086: {in the supercritical state}
- B01J 2219/0236: Metal based
- Y02E 30/30: Nuclear fission reactors
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A process for hydrothermal oxidation of combustible materials in which, during at least a part of the oxidation, corrosive material is present and makes contact with at least a portion of the apparatus over a contact area on the apparatus. At least a portion of the contact surface area comprises iridium, iridium oxide, an iridium alloy, or a base metal overlaid with an iridium coating. Iridium has been found to be highly resistant to environments encountered in the process of hydrothermal oxidation. Such environments typically contain greater than 50 mole percent water, together with oxygen, carbon dioxide, and a wide range of acids, bases and salts. Pressures are typically about 27.5 to about 1000 bar while temperatures range as high as 800.degree. C.

## Claims

### Claim 1

A process for hydrothermal oxidation of combustible material in a hydrothermal oxidation apparatus, in which, during at least part of the oxidation, corrosive material is present and contacts the apparatus over a contact area on the apparatus, the process comprising:
contacting in an aqueous phase the combustible material and an oxidizing agent under conditions suitable to cause oxidation of the combustible material;
wherein the oxidation is at a temperature in the range of about 300.degree. C. to about 800.degree. C. and at pressures from about 27.5 bar (400 psi) to about 1000 bar (15,000 psi); and
wherein the contact area comprises iridium to provide corrosion resistance from said corrosive material in said contact area.

### Claim 2 (depends on 1)

The process of claim 1, wherein the corrosive material comprises at least one moiety selected from the group consisting of Cl, SO.sub.4 and OH and at least one moiety selected from the group consisting of H, Na, K, Ca, Mg, Ce, Pb and Zn.

### Claim 3 (depends on 2)

The process of claim 2, wherein the corrosive material comprises (i) at least one selected from the group consisting of HCl, H.sub.2 SO.sub.4, NaOH, Na.sub.2 CO.sub.3 and (ii) a sodium salt.

### Claim 4 (depends on 1)

The process of claim 1, wherein the aqueous phase containing the corrosive material and oxidizing agent contains greater than 50 mole percent water.

### Claim 5 (depends on 4)

The process of claim 4, wherein the aqueous phase further contains oxygen, carbon dioxide, and at least one selected from the group consisting of acids, bases and salts.

### Claim 6 (depends on 1)

The process of claim 1, wherein the oxidation apparatus is a reactor selected from the group consisting of vessel reactors, hydraulic column reactors, and pipe reactors.

### Claim 7 (depends on 1)

The process of claim 1, wherein the contact area comprises a base metal overlaid with an iridium coating.

### Claim 8

A process for hydrothermal oxidation of combustible material in a hydrothermal oxidation apparatus, in which, during at least part of the oxidation, corrosive material is present and contacts the apparatus over a contact area on the apparatus, the process comprising:
contacting in an aqueous phase the combustible material and an oxidizing agent under conditions suitable to cause oxidation of the combustible material;
wherein the oxidation is at a temperature in the range of about 300.degree. C. to about 800.degree. C. and at pressures from about 27.5 bar (400 psi) to about 1000 bar (15,000 psi); and
wherein the contact area comprises an iridium based protective layer to provide corrosion resistance from said corrosive material in said contact area.

### Claim 9 (depends on 8)

The process of claim 8, wherein the corrosive material comprises at least one moiety selected from the group consisting of Cl, SO.sub.4 and OH, and at least one moiety selected from the group consisting of H, Na, K, Ca, Mg, Ce, Pb and Zn.

### Claim 10 (depends on 9)

The process of claim 9, wherein the corrosive material comprises (i) at least one selected from the group consisting of HCl, H.sub.2 SO.sub.4, NaOH, Na.sub.2 CO.sub.3 and (ii) a sodium salt.

### Claim 11 (depends on 8)

The process of claim 8, wherein the aqueous phase containing the corrosive material and oxidizing agent contains greater than 50 mole percent water.

### Claim 12 (depends on 11)

The process of claim 11, wherein the aqueous phase further contains oxygen, carbon dioxide, and at least one selected from the group consisting of acids, bases and salts.

### Claim 13 (depends on 8)

The process of claim 8, wherein the oxidation apparatus is a reactor selected from the group consisting of vessel reactors, hydraulic column reactors, and pipe reactors.

### Claim 14 (depends on 8)

The process of claim 8, wherein the iridium protective layer is formed in-situ by contacting an iridium surface with an oxidizing agent under conditions suitable to cause oxidation of the iridium surface.

### Claim 15 (depends on 14)

The process of claim 14, wherein the oxidation of the iridium surface comprises contacting the iridium surface with an aqueous phase which includes the oxidizing agent at a temperature of about 300.degree. C. to about 800.degree. C. and a pressure from about 27.5 bar to about 1000 bar.

### Claim 16

A process for hydrothermal oxidation of combustible material in a hydrothermal oxidation apparatus, in which, during at least part of the oxidation, corrosive material is present and contacts the apparatus over a contact area on the apparatus, the process comprising:
contacting in an aqueous phase the combustible material and an oxidizing agent under conditions suitable to cause oxidation of the combustible material;
wherein the oxidation is at a temperature in the range of about 300.degree. C. to about 800.degree. C. and at pressures from about 27.5 bar (400 psi) to about 1000 bar (15,000 psi); and
wherein the contact area comprises an iridium alloy to provide corrosion resistance from said corrosive material in said contact area.

### Claim 17 (depends on 16)

The process of claim 16, wherein the corrosive material comprises at least one moiety selected from the group consisting of Cl, SO.sub.4 and OH, and at least one moiety selected from the group consisting of H, Na, K, Ca, Mg, Ce, Pb and Zn.

### Claim 18 (depends on 17)

The process of claim 17, wherein the corrosive material comprises (i) at least one selected from the group consisting of HCl, H.sub.2 SO.sub.4, NaOH, Na.sub.2 CO.sub.3 and (ii) a sodium salt.

### Claim 19 (depends on 16)

The process of claim 16, wherein the aqueous phase containing the corrosive material and oxidizing agent contains greater than 50 mole percent water.

### Claim 20 (depends on 19)

The process of claim 19, wherein the aqueous phase further contains oxygen, carbon dioxide, and at least one selected from the group consisting of acids, bases and salts.

### Claim 21 (depends on 16)

The process of claim 16, wherein the oxidation apparatus is a reactor selected from the group consisting of vessel reactors, hydraulic column reactors, and pipe reactors.

### Claim 22 (depends on 16)

The process of claim 16, wherein the contact area comprises a base metal overlaid with an iridium alloy coating.

### Claim 23 (depends on 16)

The process of claim 16, wherein the iridium alloy comprises an iridium platinum alloy.

### Claim 24 (depends on 23)

The process of claim 23, wherein the iridium platinum alloy comprises greater than about 50 wt. % iridium.