Method of manufacturing a composite
AssigneeSociete Europeenne de Propulsion
InventorsStephane Goujard, Pascal Dupel, Rene Pailler, Xavier Bourrat
Life of this patent
Estimating the term…
Loading patent…
AssigneeSociete Europeenne de Propulsion
InventorsStephane Goujard, Pascal Dupel, Rene Pailler, Xavier Bourrat
Estimating the term…
The pyrolytic carbon lamellar interphase is formed on the reinforcing fibers inside a chamber in which a plurality of successive cycles is performed, each cycle comprising: injecting a reaction gas in which the pyrolytic carbon precursor is selected from alkanes, excluding methane taken as a sole component, alkenes, alkynes, and aromatic hydrocarbons, and mixtures thereof; the gas is maintained inside the chamber for a first predetermined time period to form an interphase layer of controlled thickness of nanometer size; the gaseous reaction products are then evacuated during a second time period; the cycles being performed consecutively in the chamber until the thickness desired for the interphase has been obtained, thereby achieving a lamellar interphase that is highly anisotropic, whose lattice fringe texture has distorted fringes of total length (L.sub.2) not less than 4 nanometers on average with maximum values exceeding 10 nanometers.
A composite material comprising fiber reinforcement densified by a matrix and a lamellar interphase coating of anisotropic pyrolytic carbon formed between the reinforcing fibers and the matrix, wherein the lamellar interphase is constituted by a highly anisotropic pyrolytic carbon whose 00.2 lattice fringe texture has distorted fringes of total length L.sub.2 that is on average not less than 4 nanometers with a maximum value that exceeds 10 nanometers, and in which the number N of elementary layers stacked coherently along the c crystallographic axis is on average not more than 4.
Dependencies are inferred from the claim text.