Process for reducing the friction coefficient between water and surfaces of polymeric materials and resulting article
AssigneeEnichem S.p.A.
InventorsMarco Morra, Ernesto Occhiello, Fabio Gabrassi
Life of this patent
Estimating the term…
Abstract
Process for reducing the friction coefficient between water, and, surfaces of fabricated bodies made from polymeric materials, and for increasing the water repellency of said surfaces, which process comprises treating the concerned surface with a corrosive solution, and coating it with a thin layer of fluorinated polymer.
Claims4
A process for reducing the friction coefficient between water and a surface of a fabricated body manufactured from a polymeric material, and increasing the water repellency of the surface, comprising:
- (a) treating the surface of the fabricated body with a corrosive means selected from the group consisting of acid oxidizing means and alkaline means;
- and
- (b) coating the treated surface with a thin layer of fluorinated polymer obtained by plasma-induced polymerization of at least one gas phase fluorinated monomer.
A process for obtaining a fabricated body, manufactured from a polymeric material, which has a water-repellent surface and a reduced friction coefficient between a surface of the body and water, comprising:
- (a) treating the surface of the fabricated body with a corrosive means selected from the group consisting of acid oxidizing means and alkaline means, until conditions of controlled roughness are obtained, wherein the surface comprises structures of a size within the range of from 0.2 to 2 micrometers;
- and
- (b) coating the treated surface with a layer of fluorinated polymer of thickness within the range of from 1 to 1000 nm, wherein said layer of fluorinated polymer is obtained by plasma-induced polymerization of at least one fluorinated monomer.
Dependencies are inferred from the claim text.