Back to results
US 5,512,114 AGranted
One-piece single metal spinneret and method for making it
AssigneeE. I. Du Pont de Nemours and Company
InventorsMark A. Short, Thomas E. Willis
Life of this patent
Estimating the term…
Abstract
A process for making a spinneret from a single body of metal with a yield strength of more than 350 MPa involving drilling lead spinneret holes into the mass of the body, annealing only a thin layer of the body opposite the lead holes, and forming capillary spinneret holes through the annealed layer to connect with the lead holes.
Claims5
A process for making a spinneret from a one-piece single metal body exhibiting a yield strength of greater than 350 MPa and having an entrance face and an exit face comprising the steps of:
- (a) drilling at least one lead hole from the entrance face into the body;
- (b) annealing only a capillary zone of the body extending from the exit face into the body to an inner end of capillary by heating only the capillary zone to a temperature above the recrystallization temperature and below the melting point of the metal whereby the metal only in the capillary zone exhibits a yield strength of less than 350 MPa;
- (c) forming at least one capillary from the exit face, through the capillary zone, into the body, and connecting with the lead hole.