Abstract
A used lubricating oil comprising lube oil additives, including zinc dithiophosphate is reconstituted. Zinc dithiophosphate is thermally decomposed at a temperature of 400.degree. F. (204.degree. C.) to 1000.degree. F. (538.degree. C.) for a residence time of 10 to 120 minutes. The resulting oil is subjected to vacuum distillation. A zinc-free (i.e. ash free by ASTM D-482) oil is stabilized by catalytic hydrogenation or clay treating to produce a lubricating oil blending stock. About 5 to 25 vol % is recovered as a metal containing bottoms product, useful as asphalt extender. The process is carried out in the absence of chemical demetallizing.
Claims18
A process for reconstituting used lubricating oil comprising organo-metallic compounds including zinc dithiophosphate in a concentration of 0.01 to 5.0 wt %, comprising:
- (a) heating the used lubricating oil by means of direct heat exchange by admixing with a heated intermediate oil to form an admixture, said heated intermediate oil at an additive decomposition temperature of about 400.degree. F. (204.degree. C.) to 1000.degree. F. (523.degree. C.);
- (b) maintaining the admixture at the additive decomposition temperature for a residence time in the range of 10 to 120 minutes, thereby reducing the zinc dithiophosphate concentration to 0.001 wt % or less to form an intermediate oil;
- (c) heating the intermediate oil to a temperature of 400.degree. F. (204.degree. C.) to 1000.degree. F. (523.degree. C.) by means of indirect heat exchange to yield the heated intermediate oil;
- and
- (d) catalytically hydrotreating the heated intermediate oil at a hydrogen partial pressure of 200 psia (13.6 atm) to 1600 psia (108.8 atm) to yield a lubricating oil.
A process for reconstituting used lubricating oil having a zinc dithiophosphate concentration of 0.01 to 5.0 wt %, comprising the steps of:
- (a) heating the used lubricating oil by direct heat exchange by means of admixing with a heated intermediate oil at an additive decomposition temperature of about 400.degree. F. (204.degree. C.) to 1000.degree. F. (538.degree. C.) and maintaining a residence time in the range of about 10 to 120 minutes to yield an intermediate oil comprising 0.001 wt % or less zinc dithiophosphate;
- (b) heating the intermediate oil by means of indirect heat exchange to the additive decomposition temperature of 400.degree. F. (204.degree. C.) to 1000.degree. F. (538.degree. C.) to produce the heated intermediate oil;
- (c) vacuum distilling the heated intermediate oil at a distillation temperature of 400.degree. F. (204.degree. C.) to 1050.degree. F. (565.degree. C.) and a distillation pressure of 20 to 500 mm Hg, and
- (d) recovering a distillate comprising 0.001 wt % or less zinc dithiophosphate;
- and
- (e) hydrotreating the heated intermediate oil at a hydrogen partial pressure of 200 psia (13,6 atm) to 1600 psia (108.8 atm) to yield a lubricating oil.
A process for reconstituting used lubricating oil comprising organo-metallic compounds including zinc dithiophosphate in a concentration of 0.01 to 5.0 wt %, comprising:
- (a) heating the used lubricating oil by means of direct heat exchange by admixing with a heated intermediate oil to form an admixture, said heated intermediate oil at an additive decomposition temperature of about 400.degree. F. (204.degree. C.) to 1000.degree. F. (523.degree. C.);
- (b) maintaining the admixture at the additive decomposition temperature for a residence time in the range of 10 to 120 minutes, thereby reducing the zinc dithiophosphate concentration to 0,001 wt % or less to form an intermediate oil;
- (c) heating the intermediate oil to a temperature of 400.degree. F. (204.degree. C.) to 1000.degree. F. (523.degree. C.) by means of indirect heat exchange to yield the heated intermediate oil;
- and
- (d) clay treating the heated intermediate oil to yield a lubricating oil.
A process for reconstituting used lubricating oil having a zinc dithiophosphate concentration of 0.01 to 5.0 wt %, comprising the steps of:
- (a) heating the used lubricating oil by direct heat exchange by means of admixing with a heated intermediate oil at an additive decomposition temperature of about 400.degree. F. (204.degree. C.) to 1000.degree. F. (538.degree. C.) and maintaining a residence time in the range of about 10 to 120 minutes to yield an intermediate oil comprising 0,001 wt % or less zinc dithiophosphate;
- (b) heating the intermediate oil by means of indirect heat exchange to the additive decomposition temperature of 400.degree. F. (204.degree. C.) to 1000.degree. F. (538.degree. C.) to produce the heated intermediate oil;
- (c) vacuum distilling the heated intermediate oil at a distillation temperature of 400.degree. F. (204.degree. C.) to 1050.degree. F. (565.degree. C.) and a distillation pressure of 20 to 500 mm Hg, and
- (d) recovering a distillate comprising 0,001 wt % or less zinc dithiophosphate;
- and
- (e) clay treating the heated intermediate oil to yield a lubricating oil.