# US 5,445,890 A · Bullet resistant glass/glass, glass/plastic, and plastic/plastic laminate composites

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,445,890 A
- Document ID: US5445890A
- Status: Granted
- Kind: A
- Application number: 08/254,879
- Filed: 1994-06-06
- Granted: 1995-08-29
- Earliest claimed: 1992-06-22
- Assignees: Resikast Corporation
- Inventors: Charles E. Bayha; H. Arne Sudlow
- Web page: https://patentgrep.com/patent/US5445890A

## CPC

- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 17/10018: {comprising only one glass sheet}
- B32B 17/10779: {containing polyester}
- B32B 27/36: comprising polyesters
- B32B 27/365: {comprising polycarbonates}
- C08F 283/01: on to unsaturated polyesters {(C08F283/004 takes precedence)}
- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- C09J 167/06: Unsaturated polyesters having carbon-to-carbon unsaturation
- F41H 5/0407: {Transparent bullet-proof laminates}{informative reference: layered products essentially comprising glass in general B32B17/06, e.g. B32B17/10009; manufacture or composition of glass, e.g. joining glass to glass C03; permanent multiple-glazing windows, e.g. with spacing therebetween, E06B3/66}
- B32B 2367/00: Polyesters, e.g. PET, i.e. polyethylene terephthalate
- B32B 2369/00: Polycarbonates
- B32B 2571/02: defensive, e.g. armour plates or anti-ballistic clothing
- Y10T 428/31507: Of polycarbonate
- Y10T 428/31616: Next to polyester [e.g., alkyd]
- Y10T 428/3162: Cross-linked polyester [e.g., glycerol maleate-styrene, etc.]
- Y10T 428/31786: Of polyester [e.g., alkyd, etc.]
- Y10T 428/31794: Of cross-linked polyester
- Y10T 428/31797: Next to addition polymer from unsaturated monomers
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- F41H: ARMOUR; ARMOURED TURRETS; ARMOURED OR ARMED VEHICLES; MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

This invention relates to multiple glass/plastic laminates for ballistic resistant and security applications. The laminates typically comprise a glass lite and a plastic sheet, such as polycarbonate, bonded with an adhesive based on a novel solvent free thermosetting alkyd resin. Subsequent layers can be polycarbonate sheets and/or acrylic sheets and glass lites with the adhesive layer separating the lites and sheets. Further, this invention relates to a vertical liquid pour process which enables the rapid manufacture of bullet resistant glass/plastic laminates without the need for expensive ultra-violet or heat curing ovens. The adhesive cures at temperatures ranging from 60.degree. F. to 90.degree. F. High temperature and high pressure treatments are unnecessary. Laminates produced in this manner with adhesive interlayer will pass all intended ballistic or security tests within a 12 hour period.

## Claims

### Claim 1

A glass laminate composite, comprising:
at least two parallel sheets of glass joined by a layer of adhesive polyester prepared by cross-linking a pre-polymer, said pre-polymer prepared by preparing a linear polyester oligomer by reacting a mixture comprising at least one dibasic acid selected from the group consisting of adipic acid, phthalic anhydride, anhydride and maleic anhydride with at least one diol selected from the group consisting of dipropylene glycol and 2-methyl-1,3-propanediol to obtain a linear polyester oligomer having a molecular weight between about 900 and 1,200 measured by gel permeation chromatography;
adjusting the refractive index of said linear polyester oligomer to the refractive index of float glass by adding propylene glycol to said mixture of said dibasic acid and said diol;
and thinning said linear polyester oligomer with at least one monomer capable of cross-linking said linear polyester, said at least one monomer containing at least 60% by weight of t-butyl styrene, to obtain an adhesive polyester pre-polymer.

### Claim 2 (depends on 1)

The glass laminate composite as set forth in claim 1, including adding a second polyester oligomer to said mixture prepared by reacting adipic acid, 2-methyl-1,3-propane-diol and propylene glycol to obtain a linear oligomer having a molecular weight of about 1000, and reacting said linear oligomer with (C.sub.2 H.sub.5 O).sub.4 Si and obtain a said second polyester oligomer having a molecular weight of about 3000.

### Claim 3 (depends on 1)

The glass laminate composite set forth in claim 1, including at least one plastic sheet in parallel relation and spaced between said at least two parallel glass sheets, said plastic sheet joined to each of said glass sheets by a layer of said adhesive polyester.

### Claim 4 (depends on 1)

The glass laminate composite set forth in claim 1, wherein said at least one monomer includes dibromostyrene.

### Claim 5

A glass/plastic laminate, comprising:
at least one plastic sheet in parallel relation and spaced from at least one glass sheet, said plastic sheet joined to said glass sheet by a layer of adhesive polyester prepared by cross-linking a pre-polymer, said pre-polymer prepared by preparing a linear polyester oligomer by reacting a mixture comprising at least one dibasic acid selected from the group consisting of adipic acid, phthalic anhydride, nadic anhydride and maleic anhydride with at least one diol selected from the group consisting of dipropylene glycol and 2-methyl-1,3-propanediol to obtain a linear polyester oligomer having a molecular weight between about 900 and 1,200 measured by gel permeation chromatography;
adjusting the refractive index of said linear polyester oligomer to the refractive index of float glass by adding propylene glycol to said mixture of said dibasic acid and said diol;
and thinning said linear polyester oligomer with at least one monomer capable of cross-linking said linear polyester, said at least one monomer containing at least 60% by weight of t-butyl styrene, to obtain an adhesive polyester pre-polymer.

### Claim 6 (depends on 5)

The glass/plastic laminate as set forth in claim 5, including adding a second polyester oligomer to said mixture prepared by reacting adipic acid, 2-methyl-1,3-propane-diol and propylene glycol to obtain a linear oligomer having a molecular weight of about 1000, and reacting said linear oligomer with (C.sub.2 H.sub.5 O).sub.4 Si and obtain a said second polyester oligomer having a molecular weight of about 3000.

### Claim 7 (depends on 5)

The glass/plastic laminate as set forth in claim 5, including at least one additional plastic sheet in parallel relation and spaced between said at least one plastic sheet and said at least one glass sheet, said at least one additional plastic sheet joined to each of said at least one plastic sheet and said at least one glass sheet by a layer of said adhesive polyester.

### Claim 8 (depends on 5)

The glass/plastic laminate as set forth in claim 5, wherein said at least one monomer includes dibromostyrene.

### Claim 9

A plastic/plastic laminate, comprising:
at least two parallel plastic sheets joined to each other by a layer of adhesive polyester resin prepared by cross-linking a pre-polymer, said pre-polymer prepared by preparing a linear polyester oligomer by reacting a mixture comprising at least one dibasic acid selected from the group consisting of adipic acid, phthalic anhydride, nadic anhydride and maleic anhydride with at least one diol selected from the group consisting of dipropylene glycol and 2-methyl-1,3-propanediol to obtain a linear polyester oligomer having a molecular weight between about 900 and 1,200 measured by gel permeation chromatography;
adjusting the refractive index of said linear polyester oligomer to the refractive index of float glass by adding propylene glycol to said mixture of said dibasic acid and said diol;
and thinning said linear polyester oligomer with at least one monomer capable of cross-linking said linear polyester, said at least one monomer containing at least 60% by weight of t-bytyl styrene, to obtain an adhesive polyester pre-polymer.

### Claim 10 (depends on 9)

A plastic/plastic laminate as set forth in claim 9, including adding a second polyester oligomer to said mixture prepared by reacting adipic acid, 2-methyl-1,3-propane-diol and propylene glycol to obtain a linear oligomer having a molecular weight of about 1000, and reacting said linear oligomer with (C.sub.2 H.sub.5 O).sub.4 Si and obtain a said second polyester oligomer having a molecular weight of about 3000.

### Claim 11 (depends on 9)

The plastic/plastic laminate as set forth in claim 9, including at least one plastic sheet in parallel relation and spaced between said at least two parallel plastic sheets, said plastic sheets joined to each other by a layer of said adhesive polyester resin.

### Claim 12 (depends on 9)

The plastic/plastic laminate as set forth in claim 9, wherein said at least one monomer includes dibromostyrene.