Polyester bottles
AssigneeICI Chemical Industries PLC
InventorNeil Tindale
Life of this patent
Estimating the term…
Abstract
Bottles can be made, especially by extrusion stretch blow moulding, using a thermoplastic polymer composition comprising a polymer, preferably a polyester, which contains metal particles especially of sb, which intrinsically absorb radiation in the wavelength region 500 nm to 2000 nm, in a quantity such that the reheat time of the polymer is less than the reheat time of the polymer in the absence of that quantity of particles. A method of making such metal containing polymer compositions by reducing a metal compound in situ is also described.
Claims6
An injection moulded bottle preform which comprises a thermoplastic polymer composition comprising a polymer which contains metal particles, which are sufficiently fine for them not to be visible to the eye and which intrinsically absorb radiation in the wavelength region 500 nm to 2000 nm, in a quantity in the range 10 to 300 ppm based on the weight of the polymer such that the reheat time of the polymer is less than the reheat time of the polymer in the absence of the particles.
An injection stretch blow moulded carbonated beverage bottle, the walls of which are made of a polyethylene terephthalate polymer which contains particles of metallic antimony which are sufficiently fine for them not to be visible to the eye and which intrinsically absorb radiation in the wavelength region 500 nm to 2000 nm, in a quantity in the range of 10 to 100 ppm based on the weight of the polymer such that the reheat time of the polymer is less than the reheat time of the polymer in the absence of the particles.
An injection moulded bottle preform the walls of which are made of a polyethylene terephthalate polymer which contains particles of metallic antimony, which are sufficiently fine for them not to be visible to the eye and which intrinsically absorb radiation in the wavelength region 500 nm to 2000 nm, in a quantity in the range 10 to 100 ppm based on the weight of the polymer such that the reheat time of the polymer is less than the reheat time of the polymer in the absence of the particles.
An injection stretch blow moulded carbonated beverage bottle the walls of which are made of thermoplastic polymer composition comprising a polymer which contains metal particles, which are sufficiently fine for them not to be visible to the eye and which intrinsically absorb radiation in the wavelength region 500 nm to 2000 nm, in a quantity in the range 10 to 300 ppm based on the weight of polymer such that the reheat time of the polymer is less than the reheat time of the polymer in the absence of that quantity of particles.
Dependencies are inferred from the claim text.