Abstract
A wellbore is drilled utilizing an oil-in-water emulsion drilling fluid, optionally containing blast furnace slag. A compatible cementitious slurry containing blast furnace slag and an activator system is then introduced into the borehole and displaced up into an annulus. Generally, the cementitious slurry is prepared by adding additional blast furnace slag and an activator such as a sodium hydroxide/sodium carbonate mixture to the used drilling fluid.
Claims15
A method for drilling and cementing a well, comprising:
- combining blast furnace slag having a particle size within the range of 2,000 to 15,000 cm.sup.2 /g with an oil-in-water emulsion drilling fluid, said blast furnace slag being present in an amount within the range of 1 to 100 lbs/bbl of said drilling fluid plus blast furnace slag;
- utilizing said drilling fluid in a well drilling operation to form a borehole to produce a used drilling fluid;
- diluting at least a portion of said used drilling fluid to an extent that on addition of blast furnace slag thereto, the final density of the diluted drilling fluid will be within the range of 30% less to 70% more than the original density;
- combining the additional blast furnace slag and an activator with said used drilling fluid to produce a cementitious slurry;
- disposing a pipe within said borehole;
- passing said cementitious slurry down said pipe;
- and
- displacing said cementitious slurry up into an annulus surrounding said pipe.
5 more elements
A method for drilling and cementing a well, comprising:
- drilling a wellbore utilizing an oil-in-water emulsion drilling fluid containing seawater, thus producing a used drilling fluid;
- diluting at least a portion of said used drilling fluid to an extent such that on addition of blast furnace slag thereto, the final density of the diluted drilling fluid will be within the range of 30% less to 70% more than the original density,
- combining the blast furnace slag and an activator with a portion of said used drilling fluid to produce a cementitious slurry , said activator being a mixture of sodium hydroxide and sodium carbonate, and wherein 5 to 25 wt% of said blast furnace slag has an ultrafine particle size;
- disposing a pipe within said borehole;
- passing said cementitious slurry down said pipe;
- and
- displacing said cementitious slurry up into an annulus surrounding said pipe.