# US 5,354,536 A · Monolithic, fully dense silicon carbide material, method of manufacturing and end uses

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,354,536 A
- Document ID: US5354536A
- Status: Granted
- Kind: A
- Application number: 08/115,678
- Filed: 1993-09-03
- Granted: 1994-10-11
- Earliest claimed: 1993-03-11
- Assignees: Cercom, Inc.
- Inventors: Andre Ezis
- Web page: https://patentgrep.com/patent/US5354536A

## CPC

- C04B 35/575: obtained by pressure sintering
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A silicon carbide material is made following a procedure including hot pressing to provide a finished product having a microstructure with an optimal grain size of less than 7 micrometers. The material exhibits a dominant failure mode of intergranular fracture requiring significant energy for crack propagation. The method of manufacturing is cost-effective by allowing the use of "dirty" raw materials since the process causes impurities to segregate at multi-grain boundary junctions to form isolated pockets of impurities which do not affect the structural integrity of the material. End uses include use as protective projectile-resistant armor.

## Claims

### Claim 1

A process for making a silicon carbide ceramic material including the steps of:
a) preparing a powder mix consisting of at least 92%, by weight, pure Silicon Carbide powder, said Silicon Carbide powder comprising alpha-type SiC or beta-type SiC, said powder having an average particle diameter of 0.3 to 3 micrometers;
b) adding to said powder a densification agent in a ratio of from 0.1% up to 0.25%, by weight, of densification agent for each m.sup.2 /g of surface area of said powder to form a powder mix;
c) homogenizing said powder mix and densification agent utilizing either a dry procedure or a wet mill process;
d) subjecting homogenized powder mix and densification agent to a hot pressing operation including the step of obtaining a state of substantially closed porosity of said material before temperature exceeds 1900.degree. C. whereby said densification agent is precluded from volatizing and is thereby captured within said material; and
e) cooling said homogenized powder mix and densification agent, said material exhibiting intergranular fracture.

### Claim 2 (depends on 1)

The process of claim 1, wherein said powder mix includes, by weight, from 0.01% to 2% Iron, from 0.01% to 1.5% Aluminum, from 0.1% to 2% free Carbon, from 0.02% to 3% Silicon Dioxide and from 0.01% to 0.15% free Silicon.

### Claim 3 (depends on 1)

The process of claim 1, wherein said densification agent comprises Aluminum Nitride.

### Claim 4 (depends on 3)

The process of claim 3, wherein said Aluminum Nitride is coated with a protective film.

### Claim 5 (depends on 1)

The process of claim 1, wherein said homogenizing step includes use of ethanol, methanol or isopropyl alcohol or a ketone solvent including methyl ethyl ketone.

### Claim 6 (depends on 1)

The process of claim 1, wherein said dry procedure includes the step of milling for 5-8 hours.

### Claim 7 (depends on 1)

The process of claim 1, wherein said dry procedure includes the step of drying for about 20 hours.

### Claim 8 (depends on 1)

The process of claim 1, wherein said dry procedure includes a mixing cycle including alternating periods with an intensifier on and off.

### Claim 9 (depends on 1)

The process of claim 1, wherein said wet mill process includes the step of screening through mesh.

### Claim 10 (depends on 1)

The process of claim 1, wherein said hot pressing operation includes the step of gradually increasing temperature from 1630.degree. C. to over 2000.degree. C. while concurrently increasing pressure from 380 psi to 1900 psi.

### Claim 11 (depends on 10)

The process of claim 10, wherein said hot pressing operation includes the step of achieving at least 80% of theoretical density of said ceramic material before said temperature exceeds 1900.degree. C.