# US 5,350,468 A · Process for producing amorphous alloy materials having high toughness and high strength

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,350,468 A
- Document ID: US5350468A
- Status: Granted
- Kind: A
- Application number: 07/939,210
- Filed: 1992-09-02
- Granted: 1994-09-27
- Earliest claimed: 1991-09-06
- Assignees: Tsuyoshi Masumoto; Akihisa Inoue; Yoshida Kogyo K.K.
- Inventors: Tsuyoshi Masumoto; Akihisa Inoue
- Web page: https://patentgrep.com/patent/US5350468A

## CPC

- C22C 45/10: with molybdenum, tungsten, niobium, tantalum, titanium, or zirconium {or Hf} as the major constituent
- C22C 45/00: Amorphous alloys (making amorphous non-ferrous alloys C22C1/11)
- C22C 45/08: with aluminium as the major constituent
- C22F 1/00: Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working (apparatus for mechanical working of metal B21, B23, B24)
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/06: of magnesium or alloys based thereon
- C22F 1/183: {of titanium or alloys based thereon}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A process for producing amorphous alloy materials having high toughness and high strength from various alloy powders, thin ribbons or bulk materials consisting of an amorphous phase by heating them to a temperature at which intermetallic compounds or other compounds are not produced. During this heating, fine crystal grains consisting of a supersaturated solid solution made of a main alloying element and additive elements and having a mean grain diameter of 5 nm to 500 nm are precipitated and uniformly dispersed in a volume percentage of 5 to 50% throughout an amorphous matrix. In the process, when deformation, pressing or other working is simultaneously conducted with the heating, consolidation or combining of the resultant alloy materials can also be effected in the same production procedure. The amorphous alloy used in the production process preferably comprises Al, Mg or Ti as a main element and, as additive elements, rare earth elements and/or other elements.

## Claims

### Claim 1

A process for producing an amorphous alloy material having high toughness and high strength, which comprises heating an amorphous alloy in the form of powder, thin ribbons or bulk shapes consisting of an amorphous phase up to a temperature at which intermetallic compounds or other compounds are not formed while subjecting the amorphous alloy being heated to deformation-forming, pressing or other working, and thereby causing precipitation and uniform dispersion of crystal grains consisting of a supersaturated solid solution made of a main element and additive elements and having a mean diameter of 5 nm to 500 nm in a volume percentage of 5 to 50% in an amorphous matrix, and simultaneously effecting consolidation-forming or combining.

### Claim 2 (depends on 1)

A process as claimed in claim 1 in which the amorphous alloy is a Ti-based amorphous alloy consisting of Ti as a main element and rare earth elements, including Y and Mm (misch metal) consisting of a mixture of rare earth elements, and/or Fe and Si as additive elements.

### Claim 3 (depends on 1)

A process as claimed in claim 1 in which the amorphous alloy is an Al-based amorphous alloy consisting of, in atomic percentages, 85 to 99.8% Al, 0.1 to 5% of at least one element selected from the group consisting of rare earth elements including Y and Mm (misch metal) consisting of a mixture of rare earth elements as primary additive elements of the additive elements and up to 10% of at least one element selected from the group consisting of Ni, Fe, Co and Cu as secondary additive elements of the additive elements, with the proviso that the total content of the rare earth elements including Y and Mm is not more than the total content of the other additive elements.

### Claim 4 (depends on 3)

A process as claimed in claim 3 in which Al as the main element of the Al-based amorphous alloy is partially substituted in the range of 0.2 to 3 atomic % by at least one element selected from the group consisting of Ti, Mn, Mo, Cr, Zr, V, Nb and Ta.

### Claim 5 (depends on 1)

A process as claimed in claim 1 in which the amorphous alloy is a Mg-based amorphous alloy consisting of, in atomic percentages, 80 to 91% Mg, 8 to 15% of at least one element selected from the group consisting of Cu, Ni, Sn and Zn as primary additive elements of the additive elements and 1 to 5% of at least one element selected from the group consisting of Al, Si and Ca as secondary additive elements of the additive elements.

### Claim 6 (depends on 1)

A process as claimed in claim 1 in which the amorphous alloy is a Mg-based amorphous alloy consisting of, in atomic percentages, 80 to 91% Mg, 8 to 15% of at least one element selected from the group consisting of Cu, Ni, Sn and Zn as primary additive elements of the additive elements and 1 to 5% of at least one element selected from the group consisting of rare earth elements including Y and Mm (misch metal) consisting of a mixture of rare earth elements as secondary additive elements of the additive elements.

### Claim 7 (depends on 6)

A process as claimed in claim 6 in which Mg as the main element of the Mg-based amorphous alloy is partially substituted in the range of 1 to 5 atomic % by at least one element selected from the group consisting of Al, Si and Ca.

### Claim 8 (depends on 2)

A process as claimed in claim 2 in which the additive elements are Fe and Si.

### Claim 9 (depends on 2)

A process as claimed in claim 2 in which said temperature ms in the range of 573.degree.-1073.degree. K.

### Claim 10 (depends on 3)

A process as claimed in claim 3 in which said temperature is in the range of 373.degree.-573.degree. K.