# US 5,347,766 A · Method for polishing surface of transparent substrate layer of color filter unit

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,347,766 A
- Document ID: US5347766A
- Status: Granted
- Kind: A
- Application number: 07/923,358
- Filed: 1992-07-16
- Granted: 1994-09-20
- Earliest claimed: 1991-07-18
- Assignees: Mitsui Toatsu Chemicals, Inc.
- Inventors: Kazuyoshi Komatsu; Osamu Narimatsu; Yasuo Takemura; Yoko Takeuchi; Susumu Waki
- Web page: https://patentgrep.com/patent/US5347766A

## CPC

- B24B 13/01: Specific tools, e.g. bowl-like; Production, dressing or fastening of these tools
- B24B 13/015: of television picture tube viewing panels, headlight reflectors or the like
- G02F 1/133514: {Colour filters}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

The present invention provides a method for polishing the surface of the transparent substrate layer of a color filter unit comprising a transparent substrate layer, a color filter layer, a protective film layer and a transparent electrode layer, which method comprises attaching, to the surface of the transparent electrode layer, a pressure-sensitive tape consisting of a base film layer and a pressure-sensitive adhesive layer giving substantially no staining to said surface of the transparent electrode layer, formed on one surface of the base film layer, as well as a pressure-sensitive tape used in the method. When the surface of the transparent substrate layer is polished according to the present method, there occurs no breakage of the color filter unit. Further, there occurs no staining of the surface of the transparent electrode layer owing to the adhesion of residual pressure-sensitive adhesive, abrasive, polishing refuse, etc. Consequently, a color filter unit giving a good image clearness can be obtained at high productivity.

## Claims

### Claim 1

A method for polishing a surface of a transparent substrate layer of a color filter unit comprising a transparent substrate layer, a color filter layer, a protective film layer and a transparent electrode layer, which method comprises attaching, to a surface of the transparent electrode layer, a pressure-sensitive tape consisting of a base film layer selected from a single layer film or a multi-layer film and a pressure-sensitive adhesive layer which gives substantially no staining to the surface of the transparent electrode layer, and polishing the surface of the transparent substrate layer of the color filter unit.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the pressure-sensitive adhesive layer which gives substantially no staining to the surface of the transparent electrode layer results in
ratios of integral of carbon (C), potassium (K), sodium (Na) and chlorine (Cl) wavelength intensities to an integral of indium (In) wavelength intensity equal to 0.1 or less (C/In), 0.03 or less (K/In), 0.03 or less (Ka/In) and 0.03 or less (Cl/In), these ratios being obtained by analysis to the survey scan spectrum method of ESCA (electron spectroscopy for chemical analysis) of the surface of the transparent electrode layer after a treatment that comprises the steps of: attaching the pressure-sensitive adhesive layer to the surface of the transparent electrode layer, the surface of the transparent electrode layer being free of foreign matter; letting stand for 24 hours in an atmosphere controlled to a temperature of 23.degree. C. .+-.2.degree. C. and a relative humidity of 50% .+-.5%; and peeling the pressure-sensitive adhesive layer from the surface of the transparent electrode layer.

### Claim 3 (depends on 2)

A method according to claim 2, wherein the pressure-sensitive adhesive layer comprises acrylic resin type adhesive.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the base film layer formed the pressure-sensitive adhesive layer has a hardness (Shore D) of 80 or less.

### Claim 5 (depends on 4)

A method according to claim 4, wherein the base film layer comprises an ethylene-vinyl acetate copolymer film, a polyethylene terephthalate film, a polyvinyl chloride film, a polyethylene film or a polypropylele film.