Lightweight aggregate from flyash and sewage sludge
AssigneeWisconsin Electric Power Company
InventorsTimothy M. Nechvatal, Glenn A. Heian
Life of this patent
Estimating the term…
Loading patent…
AssigneeWisconsin Electric Power Company
InventorsTimothy M. Nechvatal, Glenn A. Heian
Estimating the term…
A method is shown for producing a lightweight aggregate by treating flyash and sewage sludge. The flyash and sewage sludge are mixed together and then agglomerated into pellets, with or without the use of a binder. The pellets may be coated and then are dried. The dried pellets are introduced into a rotary kiln in a direction that is co-current with the flow of fuel and air through the kiln. The pellets in the kiln will be indurated and will experience complete calcination as well as varying degrees of pyrolizing and sintering. The product of the kiln is a nodular material having a low density but with a hard and porous structure. The product of the kiln is feed to a cooler. The flyash sewage sludge mixture has a significant fuel value that is usable in the kiln. Furthermore, the fuel value available in the kiln off-gases may be used for drying the materials.
A lightweight aggregate consisting of a porous nodular heat-hardened agglomerate of 35-80% by dry weight of flyash and 20-65% by dry weight of uncombusted sewage sludge having an organic content.
A lightweight aggregate having a maximum loose density of between 55 and 70 pounds per cubic foot, said aggregate consisting essentially of a heat-hardened agglomerate of 35-80% by dry weight of flyash and 20-65% by dry weight of uncombusted sewage sludge and that has a hard and porous nodular structure.
A lightweight aggregate consisting essentially of a porous nodular heat-hardened agglomerate of 35-80% by dry weight of flyash and 20-65% by dry weight of uncombusted sewage sludge having an organic content.