Process for improving the elasticity of a ski edge made of corrosion-resistant martensitic chrome steel, consisting of pre-stretching the edge, and for the manufacture of a ski incorporating edges so produced.
Claims9
Process for improving the elasticity of a ski edge made of corrosion-resistant martensitic chrome steel, wherein the process comprises providing corrosion-resistant martensitic chrome steel having a configuration serving as a ski edge and exerting traction on said ski edge in a longitudinal direction so as to pre-stretch said ski edge beyond its elastic limit in order to impart to it an irreversible longitudinal deformation.
Process for the manufacture of a ski comprises providing corrosion-resistant martensitic chrome steel having a configuration serving as a ski edge, exerting traction on said ski edge in a longitudinal direction so as to pre-stretch said ski edge beyond its elastic limit in order to impart to it an irreversible longitudinal deformation, providing a ski and incorporating said pre-stretched ski edge on said ski.
Dependencies are inferred from the claim text.