Monomer recovery from polymeric materials
AssigneeBattelle Memorial Institute
InventorsMark A. Paisley, Robert D. Litt
Life of this patent
Estimating the term…
Abstract
A method is described for the recovery of high yields of monomers from waste and scrape polymeric materials with minimal amounts of char and tar. The process involves heating the polymer at a heating rate of at least 500.degree. C./sec in a flow-through reactor. Heating is accomplished by contacting the polymer with a heat transfer material such as hot incandescent sand. A flow-through reactor is used to provide the high heating rates and short reactor residence times for the monomer product. The flow through reactor may be a circulating fluidized bed reactor, an entrainment reactor, a cyclonic reactor or a gravity reactor.
Claims18
A process for monomer recovery from a polymeric material comprising heating said polymeric material in a flow-through reactor by means of a heat transfer material at a heating rate of at least 500.degree. C./second to recover a monomeric component of said polymeric material.
A process for monomer recovery from a polymeric material comprising heating said polymeric material in a pyrolyzer at a rate of at least 500.degree. C./second to recover a monmoeric component of said polymeric material essentially without the formation of solid carbon and non-monomeric liquid components by contacting for less than 2 seconds said polymeric material with a heat-transfer material that circulates through said pyrolyzer.
A process for monomer recovery comprising heating a polymeric material at a rate of at least about 500.degree. C./sec to a pyrolysis temperature of about 650.degree. C. to about 1000.degree. C. in less than about 2 seconds in a reactor by means of a heat-transfer material that circulates through said reactor.
Dependencies are inferred from the claim text.