Ion exchange materials produced from hydrolyzed, debituminized, sulfonated peat
AssigneeBemidji State University Foundation
InventorsGerald H. Morine, Steven A. Spigarelli
Life of this patent
Estimating the term…
Abstract
An improved process for preparing a cation exchange material from peat selected from sphagnum or reed-sedge peat for improving the ion exchange capability of the peat. The raw peat is initially dried and ground to a particle size of less than about one millimeter, after which the particulate material is hydrolyzed in an acid solution of moderate strength for separation of soluble components. The hydrolyzed material is then refluxed in an organic solvent, such as a mixture of 2-propanol and toluene in a 1:2 volume ratio. Following removal of residual solvent, the peat is reacted with warm concentrated sulfuric acid, and thereafter ground or milled to a desirable particle size.
Claims5
The method of preparing a cation exchange material from peat which includes the steps of:
- (a) passing a supply of dried peat through a treating chamber to reduce the particle size to less than about 1 mm;
- (b) hydrolyzing the particulate peat in an aqueous solution having a pH of less than about 2 to separate the soluble components therefrom;
- (c) refluxing the residual hydrolyzed peat in an organic solvent selected from the group consisting of petroleum ether, 2-butanone, 2-propanol, toluene, and mixtures of 2-propanol and toluene to extract solvent soluble bitumen therefrom, and thereafter drying the refluxed peat of residual solvent;
- and
- (d) thereafter reacting the solvent-free treated peat with concentrated sulfuric acid at a temperature greater than about 100 degrees C. for at least about one hour, and thereafter removing the remaining sulfuric acid.
A cation exchange material prepared by the processing steps of:
- (a) passing a supply of dried peat through a treating chamber to reduce the particle size to less than about 1 mm;
- (b) hydrolyzing the particulate peat in an aqueous solution having a pH of less than about 2 to separate the soluble components therefrom;
- (c) refluxing the residual hydrolyzed peat in an organic solvent selected from the group consisting of petroleum ether, 2-butanone, 2-propanol, toluene, and mixtures of 2-propanol and toluene to extract essentially all of the solvent bitumen therefrom, and thereafter drying the refluxed peat of residual solvent;
- and
- (d) thereafter reacting the solvent-free treated peat with concentrated sulfuric acid at a temperature greater than about 100 degrees C. for at least about one hour, and thereafter removing the remaining sulfuric acid.
Dependencies are inferred from the claim text.