Base coat stucco mortars for coating and finishing interior and exterior walls of a building
OwnerBurton K. Whatcottinventor
Life of this patent
Estimating the term…
Abstract
A stucco coating for interior and exterior walls of buildings that provides increased bonding strength over the prior art.
Claims7
A refractory combination for a base coating for mortars comprising in combination:
- approximately 90 pounds of Portland cement,
- approximately 10 pounds of hydrated lime,
- approximately 2 pounds of reinforcing fibers,
- approximately 8 pounds of polymer solids,
- approximately 3 parts of sand to 1 part of cement by volume,
- water as needed to provide a fluid workable combination, wherein
- said reinforcing fibers comprise fiberglass, and
- said polymer solids comprise styrene butadiene rubber.
A refractory combination for a high strength base coat for mortars comprising:
- approximately 90.00 pounds of Portland cement,
- approximately 10.00 pounds micro silica,
- approximately 2.00 pounds reinforcing fiber,
- approximately 2.00 ounces super plasticizer,
- approximately 15.00 pounds polymer solids,
- approximately 2:1 ratio of sand to cement by volume,
- approximately 0.50 pounds dispersant, and
- water as needed to obtain a fluid combination, wherein
- said polymer solids comprise styrene butadiene rubber.
A refractory combination for a quick setting base coat comprising:
- approximately 95.00 pounds Portland cement,
- approximately 5.00 pounds aluminite cement,
- approximately 4.00 pounds clay,
- approximately 2.00 pounds reinforcing fibers,
- approximately 10.00 pounds polymer solids,
- approximately 3:1 ratio of sand to cement by volume, and
- water as needed to obtain a fluid combination, wherein
- said polymer solids comprise styrene butadiene rubber.
A refractory combination for a waterproof base coating for mortars comprising:
- approximately 80.0 pounds Portland cement,
- approximately 20.00 pounds of pozzolan,
- approximately 2.00 pounds reinforcing fibers,
- approximately 20.00 pounds polymer solids,
- approximately 0.25 pounds cellulose,
- approximately 2:1 ratio of sand to cement by volume,
- water as needed to obtain a fluid combination, and
- approximately 3.00 pounds waterproofing agent, wherein
- said polymer solids comprise styrene butadiene rubber.
A refractory combination for a pump applied base coating for mortars comprising:
- approximately 100.00 pounds Portland cement,
- approximately 10.00 pounds hydrated lime,
- approximately 15.00 pounds pozzolan,
- approximately 10.00 pounds polymer solids,
- approximately 2.00 pounds reinforcing fibers,
- approximately 3:1 ratio of said to cement by volume, and
- water as needed to obtain a fluid combination, wherein
- said polymer solids comprise styrene butadiene rubber.
A refractory combination for a lightweight nailable base coating for mortars comprising:
- approximately 80.00 pounds Portland cement,
- approximately 20.00 pounds pozzolan,
- approximately 4.00 pounds clay,
- approximately 4.00 ounces air entraining super plasticizer,
- approximately 2.00 pounds reinforcing fibers,
- approximately 10.00 pounds polymer solids,
- approximately 2.50 ft.sup.3 lightweight filler, and
- water as needed to obtain a fluid combination, wherein
- said polymer solids comprise styrene butadiene rubber.
A refractory combination for a base coating for mortars comprising in combination:
- approximately 90 pounds of Portland cement,
- approximately 10 pounds of hydrated lime,
- approximately 2 pounds of reinforcing fibers,
- approximately 8 pounds of polymer solids, and
- approximately 3 parts of sand to 1 part of cement by volume, wherein p1 said polymer solids comprise styrene butadiene rubber.
Dependencies are inferred from the claim text.