Ammonia extraction of gold and silver from ores and other materials
AssigneeSouth Dakota School of Mines & Techology
InventorsKenneth N. Han, Xinghui Meng
Life of this patent
Estimating the term…
Abstract
Gold and silver are extracted from their elemental state or from complex ores and alloys by leaching them with a solution containing ammonia, ammonium salts and one or more oxidants. The process is particularly effective for refractory gold ores including sulfide and carbonaceous ores.
Claims10
A process for extracting elemental gold and elemental silver from gold-silver ores comprising the steps of:
- I. suspending the gold-silver ore in an aqueous leach solution comprising:
- from about 2 to about 8 gram-moles per liter of ammonia;
- from about 0.1 to 2 gram-moles of ammonia salts selected from the group consisting of ammonium iodide, ammonium phosphate, ammonium bromide, ammonium carbonate, ammonium acetate and mixtures thereof;
- and
- an effective amount of an oxidant selected from the group consisting of cupric ions, manganic ions, oxygen, ozone, hypochlorite, hydrogen peroxide and mixtures thereof;
- thereby forming a suspension;
- and
- II. charging the suspension to a reaction zone;
- and
- III. heating the suspension in the reaction zone to a temperature of about 100.degree. C. to 300.degree. C. and a pressure of about 689.5 (100 psi) to 6895 kN/m.sup.2 (1000 psi) thereby forming a leach solution containing gold-ammine and silver-ammine;
- and
- IV. recovering the elemental gold and silver from the leach solution.
A process of extracting elemental gold and elemental silver from gold=silver ores comprising the steps of:
- I. grinding the gold-silver ores to produce particulate ore which passes through a No. 100 U.S. Sieve;
- and
- II. mixing the particulate ore in a reaction zone with a leach solution containing:
- from about 1 to about 8 gram-moles per liter of ammonia;
- and
- from about 0.5 to about 2 gram-moles per liter of ammonium salts selected from the group consisting of ammonium salts selected from the group consisting of ammonium iodide, ammonium phosphate, ammonium carbonate, ammonium bromide, ammonium acetate, and mixtures thereof;
- and
- an effective amount of an oxidant selected from the group from the group consisting of cupric ions, manganic ions, oxygen, ozone, hypochlorite, hydrogen peroxide and mixtures thereof;
- and
- III. then heating the material in the reaction zone to a temperature from about 100.degree. to about 300.degree. C. and a pressure from about 689.5 kN/m.sup.2 (100 psi) to about 6895.5 kN/m.sup.2 (1000 psi) thereby forming a hot leach solution containing gold-ammine and silver-ammine;
- and
- IV. cooling the hot leach solution;
- and
- V. recovering the elemental gold and silver from the leach solution.
A process for extracting elemental gold and elemental silver from gold-silver ores comprising the steps of:
- I. suspending the gold-silver ore in an aqueous leach solution comprising:
- from about 2 to about 8 gram-moles per liter of ammonia;
- a metal salt of 0.1 to 0.5 gram-moles per liter selected from the group consisting of metal-bromide, metal iodide, metal phosphate, metal carbonate and metal acetate;
- and
- from 1 to about 10 grams per liter of an oxidant selected from the group consisting of cupric ions, manganic ions, oxygen, ozone, hypochlorite, hydrogen peroxide and mixtures thereof;
- thereby forming a suspension;
- and
- II. charging the suspension to a reaction zone;
- and
- III. heating the suspension in a reaction zone to a temperature of about 100.degree. to 300.degree. C. and a pressure of about 689.5(100 psi) to 6895 kN/m.sup.2 (1000 psi) thereby forming a leach solution containing gold-ammine and silver-ammine;
- and
- IV. recovering the elemental gold and silver from the leach solution.