# US 5,304,402 A · Curtain coating method with reduced neck-in

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,304,402 A
- Document ID: US5304402A
- Status: Granted
- Kind: A
- Application number: 07/889,922
- Filed: 1992-06-02
- Granted: 1994-04-19
- Earliest claimed: 1991-06-03
- Assignees: Fuji Photo Film Co., Ltd.
- Inventors: Shouji Nishida; Yoshinobu Katagiri; Yasushi Suga
- Web page: https://patentgrep.com/patent/US5304402A

## CPC

- G03C 1/74: Applying photosensitive compositions to the base; Drying processes therefor (G03C1/496 takes precedence)
- B05C 5/008: {Slide-hopper curtain coaters}
- B05C 9/06: for applying two different liquids or other fluent materials, or the same liquid or other fluent material twice, to the same side of the work
- G03C 2001/7433: {Curtain coating}
- G03C 2001/7466: {Geometry and shape of application devices}
- G03C 2001/747: {Lateral edge guiding means for curtain coating}
- Y10S 118/04: Curtain coater
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- B05C: APPARATUS FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (spraying apparatus, atomising apparatus, nozzles B05B; plant for applying liquids or other fluent materials to objects by electrostatic spraying B05B5/08)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A film applying method in which a coating solution is applied by a solution injector having an edge guide onto a support member as a freely falling coating film, includes forming a solution contact surface of the edge guide to have one of a radius greater than 1.0 mm or a width d greater than 0.7 mm when the coating solution has at least one of a viscosity greater than 45 cp and a dynamic surface tension difference greater than 8 dyne/cm. The edge guide solution contacting surface is narrowed to have a radius less than 1.0 mm or a width d less than 0.7 mm when the coating solution has at least one of a viscosity less than 45 cp and a dynamic surface tension difference less than 8. In a second embodiment, the coating solution is prepared to have at least one of a viscosity greater than 45 cp and a dynamic surface tension difference greater than 8 dyne/cm when the solution contacting part of the edge guide has either a radius r greater than 1.0 mm or a width d greater than 0.7 mm. Alternatively, the coating solution is prepared to have at least one of a viscosity less than 45 cp and a dynamic surface tension difference less than 8 dyne/cm when the solution contacting part of the edge guide has either a radius r less than 1.0 mm or a width d less than 0.7 mm.

## Claims

### Claim 1

A curtain-film coating method for applying a coating solution onto a support member, said method comprising the steps of:
providing a solution injector having at two side ends thereof an edge guide for supporting the coating solution to apply the coating solution onto said support member as a freely falling curtain of coating film; and
forming a solution contacting surface of said edge guide to have one of a radius r greater than 1.0 mm and a width d greater than 0.7 mm when said coating solution has at least one of a viscosity .mu. greater than 45 cp and a dynamic/static surface tension difference .DELTA..sigma. greater than 8 dyne/cm,
wherein said solution contacting surface is narrowed to have a radius r less than 1.0 mm or a width d less than 0.7 mm when said coating solution has at least one of a viscosity less than 45 cp and a dynamic/static surface tension difference .DELTA..sigma. less than 8 dyne/cm.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising applying 2 cc/(cm.multidot.sec) of the coating solution by using an edge guide having a width d of 1 mm, and flowing a gelatin 2% solution containing a water:methanol ratio of 7:3 along the edge guide as an auxiliary liquid.

### Claim 3

A curtain-film coating method for applying a coating solution onto a support member, said method comprising the steps of:
providing a solution injector having at first and second ends thereof an edge guide for supporting the coating solution to apply the coating solution onto said support member as a freely falling curtain of coating film, said edge guide having a solution contacting part; and
preparing said coating solution to have at least one of a viscosity .mu. greater than 45 cp and a dynamic/static surface tension difference .DELTA..sigma. greater than 8 dyne/cm when the solution contacting part of said edge guide has one of a radius r greater than 1.0 mm and a width d greater than 0.7 mm,
wherein said coating solution is prepared to have at least one of a viscosity .mu. less than 45 cp and a dynamic/static surface tension difference .DELTA..sigma. less than 8 dyne/cm when said edge guide solution contacting part has one of a radius r less than 1.0 mm and a width d less than 0.7 mm.

### Claim 4 (depends on 3)

The method according to claim 3, wherein said coating solution comprises a gelatin water solution having a viscosity .mu. of 25 cp and contains a surface active agent comprising 30 cc/l of .alpha.-sulfosuccinic acid 2-ethyl hexyl ester sodium mixed to form the coating solution.

### Claim 5 (depends on 3)

The method according to claim 3, wherein said coating solution comprises a gelatin water solution having a viscosity of 27 cp and contains 30 cc/l of polystyrene sulfonic acid sodium.

### Claim 6 (depends on 3)

The method according to claim 3, wherein said coating solution comprises a gelatin water solution having a viscosity of 67 cp and contains 30 cc/l of polystyrene sulfonic acid sodium.

### Claim 7 (depends on 3)

The method according to claim 3, further comprising applying 2 cc/(cm.multidot.sec) of the coating solution by using an edge guide having a width d of 1 mm and flowing a gelatin 2% solution having a water:methanol ratio of 7:3 along the edge guide as an auxiliary liquid.