US 5,296,578 AGranted
Production of polysuccinimide and polyaspartic acid from maleic anhydride and ammonia
AssigneeDonlar Corporation
InventorsLarry P. Koskan, Abdul R. Y. Meah
Life of this patent
Estimating the term…
Abstract
Production of polysuccinimide by reacting maleic anhydride and ammonia at elevated temperatures. The base hydrolyzed polyaspartic acid product.
Claims11
A method of producing a polysuccinimide comprising the steps of:
- a). adding maleic anhydride and ammonia to the same reaction vessel, and
- b). heating the resulting mixture to a temperature of at least 170.degree. C., until at least a yield of polysuccinimide of at least 70% of theoretical has been produced.